Final Magnetic Moment0.009 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.439 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.287 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <0 0 1> | <0 0 1> | 262.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 262.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 314.8 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 232.2 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 205.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 209.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 209.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 262.3 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 232.2 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 102.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 262.3 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 102.6 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 205.2 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 262.3 |
Te2W (mp-22693) | <1 1 1> | <0 1 1> | 116.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 102.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 232.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 314.8 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 116.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 -1 1> | 136.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 262.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 209.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 262.3 |
BN (mp-984) | <1 1 0> | <1 -1 1> | 136.4 |
BN (mp-984) | <1 1 1> | <1 -1 1> | 136.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 314.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 -1 0> | 252.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 237.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 262.3 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 165.7 |
TiO2 (mp-2657) | <1 1 0> | <1 -1 0> | 252.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 102.6 |
C (mp-66) | <1 1 0> | <0 1 1> | 232.2 |
LaF3 (mp-905) | <0 0 1> | <0 1 1> | 232.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 262.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 262.3 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 102.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 262.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 209.9 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 209.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 314.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 314.8 |
C (mp-48) | <0 0 1> | <1 0 1> | 237.2 |
Au (mp-81) | <1 1 0> | <0 0 1> | 314.8 |
WSe2 (mp-1821) | <1 1 0> | <1 1 1> | 174.9 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 314.8 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 314.8 |
WS2 (mp-224) | <1 0 1> | <0 1 1> | 232.2 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 262.3 |
ZrO2 (mp-2858) | <1 1 -1> | <0 0 1> | 262.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TaPCl10 (mp-27788) | 0.0540 | 0.000 | 3 |
UPCl10 (mp-540927) | 0.1171 | 0.000 | 3 |
Ni(NF7)2 (mp-558988) | 0.3335 | 0.000 | 3 |
Ti(PCl6)4 (mp-685813) | 0.3542 | 0.009 | 3 |
Sn(PCl6)4 (mp-685443) | 0.3380 | 0.004 | 3 |
SiH8(NF3)2 (mp-759722) | 0.5342 | 0.000 | 4 |
SbP(Cl2F3)2 (mp-559301) | 0.4403 | 0.095 | 4 |
AsSOF9 (mp-556515) | 0.5780 | 0.044 | 4 |
MgPHO9 (mp-632723) | 0.5140 | 0.947 | 4 |
MgPHO9 (mp-720260) | 0.4984 | 0.952 | 4 |
PCl5 (mp-23228) | 0.4743 | 0.000 | 2 |
PCl5 (mp-569410) | 0.5316 | 0.006 | 2 |
NaCrH8(NF3)2 (mp-976447) | 0.5808 | 0.013 | 5 |
NaGaH8(NF3)2 (mp-865095) | 0.5784 | 0.008 | 5 |
NaInH8(NF3)2 (mp-643394) | 0.6358 | 0.028 | 5 |
SnH20C6(NCl3)2 (mp-570348) | 0.7316 | 0.071 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv P Cl |
Final Energy/Atom-3.7772 eV |
Corrected Energy-102.9324 eV
Uncorrected energy = -90.6524 eV
Composition-based energy adjustment (-0.614 eV/atom x 20.0 atoms) = -12.2800 eV
Corrected energy = -102.9324 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)