Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.094 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.813 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 249.1 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 105.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 105.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 249.1 |
BN (mp-984) | <1 1 0> | <0 1 1> | 134.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 249.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 211.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 249.1 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 211.0 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 142.6 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 156.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 249.1 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 105.5 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 105.5 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 105.5 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 249.1 |
C (mp-48) | <0 0 1> | <0 1 0> | 105.5 |
WSe2 (mp-1821) | <0 0 1> | <0 1 1> | 134.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 1 1> | 134.2 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 249.1 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 249.1 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 249.1 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 115.9 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 156.7 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 105.5 |
GaSb (mp-1156) | <1 1 1> | <0 1 1> | 134.2 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 166.1 |
Cu (mp-30) | <1 1 1> | <0 1 1> | 134.2 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 249.1 |
Fe2O3 (mp-24972) | <1 1 1> | <0 0 1> | 249.1 |
ZnTe (mp-2176) | <1 1 0> | <0 1 0> | 105.5 |
ZnTe (mp-2176) | <1 1 1> | <0 1 1> | 134.2 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 142.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 166.1 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 134.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 249.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 115.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 166.1 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 134.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 211.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 249.1 |
BN (mp-984) | <1 1 1> | <0 1 1> | 134.2 |
Fe3O4 (mp-19306) | <1 1 0> | <0 1 0> | 105.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 83.0 |
C (mp-66) | <1 1 1> | <0 1 1> | 134.2 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 166.1 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 105.5 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 166.1 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 249.1 |
PbSe (mp-2201) | <1 1 1> | <0 1 1> | 134.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba3FeS5 (mp-630328) | 0.3697 | 0.074 | 3 |
Rb3ZnBr5 (mp-505001) | 0.3202 | 0.003 | 3 |
Cs3CoI5 (mp-569323) | 0.3442 | 0.000 | 3 |
Cs3CdI5 (mp-669317) | 0.3776 | 0.005 | 3 |
Ba2SiSe4 (mp-14447) | 0.3767 | 0.000 | 3 |
KSrVO4 (mp-628859) | 0.3526 | 0.000 | 4 |
Ba3AlHO4 (mp-707218) | 0.3372 | 0.000 | 4 |
SrTlVO4 (mp-566556) | 0.4281 | 0.000 | 4 |
NaNdSiO4 (mp-13774) | 0.4241 | 0.000 | 4 |
NaLaSiO4 (mp-1020648) | 0.4283 | 0.000 | 4 |
TlBr2 (mp-27398) | 0.7189 | 0.000 | 2 |
InI2 (mp-29312) | 0.6594 | 0.000 | 2 |
InBr2 (mp-568108) | 0.6819 | 0.000 | 2 |
GaBr2 (mp-650841) | 0.7327 | 0.011 | 2 |
GaCl2 (mp-568848) | 0.6853 | 0.000 | 2 |
KCaNd(PO4)2 (mp-676934) | 0.5682 | 0.000 | 5 |
K2BiMoPO8 (mp-566924) | 0.6059 | 0.000 | 5 |
K2BiPWO8 (mp-566769) | 0.6030 | 0.001 | 5 |
NaYPO4F (mp-10804) | 0.5657 | 0.003 | 5 |
NaErPO4F (mp-10935) | 0.5756 | 0.004 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Si S |
Final Energy/Atom-5.2659 eV |
Corrected Energy-202.8398 eV
-202.8398 eV = -189.5706 eV (uncorrected energy) - 13.2692 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)