Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.502 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.046 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42mc [105] |
HallP 4c 2 |
Point Group4mm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 209.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 314.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 117.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 98.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 314.9 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 279.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 63.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 314.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 279.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 139.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 94.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 279.8 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 279.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 69.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 139.9 |
BN (mp-984) | <1 1 0> | <1 0 0> | 69.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 314.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 314.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 282.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 314.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 188.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 139.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 279.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 251.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 279.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 209.8 |
TeO2 (mp-2125) | <0 1 1> | <1 1 0> | 296.7 |
TeO2 (mp-2125) | <1 0 1> | <1 1 0> | 296.7 |
TeO2 (mp-2125) | <1 1 1> | <1 0 0> | 209.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 139.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 314.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 314.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 251.9 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 251.9 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 282.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 251.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 314.9 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 314.9 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 296.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 314.9 |
GaSe (mp-1943) | <1 0 0> | <1 1 0> | 197.8 |
BN (mp-984) | <0 0 1> | <1 1 1> | 234.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 188.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 63.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 314.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 94.1 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 63.0 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 314.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 251.9 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 279.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.04951 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.04951 | 0.00000 | 0.00000 |
0.04833 | 0.04833 | 0.03799 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.07820 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
15.08 | 0.00 | 0.00 |
0.00 | 15.08 | 0.00 |
0.00 | 0.00 | 13.84 |
Dielectric Tensor εij (total) |
||
---|---|---|
24.71 | 0.00 | 0.00 |
0.00 | 24.71 | -0.00 |
0.00 | -0.00 | 21.46 |
Polycrystalline dielectric constant
εpoly∞
14.67
|
Polycrystalline dielectric constant
εpoly
23.63
|
Refractive Index n3.83 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ge_d As |
Final Energy/Atom-4.5983 eV |
Corrected Energy-91.9659 eV
-91.9659 eV = -91.9659 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)