Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.165 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.067 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg2O + Ag2B8O13 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR32 [155] |
HallR 3 2" |
Point Group32 |
Crystal Systemtrigonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 338.8 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 95.3 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 234.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 169.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 293.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 203.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 267.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 203.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 169.4 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 293.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 338.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 338.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 305.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 169.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 285.8 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 293.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 101.7 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 169.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 135.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 203.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 267.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 169.4 |
GaSe (mp-1943) | <1 1 1> | <1 1 0> | 117.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 293.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 169.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 169.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 267.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 293.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 237.2 |
BN (mp-984) | <0 0 1> | <1 1 0> | 176.1 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 213.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 89.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 203.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 169.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 190.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 271.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 237.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 89.1 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 293.4 |
TeO2 (mp-2125) | <1 0 1> | <1 1 0> | 234.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 89.1 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 117.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 237.2 |
BN (mp-984) | <1 0 1> | <1 0 0> | 169.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 267.2 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 67.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 338.8 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 338.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 101.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-0.13838 | 0.13838 | 0.00000 | -0.31662 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.31662 | 0.13838 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.13838 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points28 |
U Values-- |
PseudopotentialsVASP PAW: B O Ag |
Final Energy/Atom-5.1467 eV |
Corrected Energy-38.1337 eV
-38.1337 eV = -36.0268 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)