Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.824 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.861 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3 [204] |
Hall-I 2 2 3 |
Point Groupm3 |
Crystal Systemcubic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 1 0> | 285.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 95.1 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 116.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 269.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 285.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 95.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 67.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 95.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 67.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 95.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 269.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 134.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 269.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 67.3 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 201.8 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 285.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 134.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 190.2 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 285.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 269.0 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 134.5 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 95.1 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 269.0 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 116.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 190.2 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 134.5 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 95.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 67.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 95.1 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 0> | 95.1 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 190.2 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 285.3 |
C (mp-66) | <1 1 0> | <1 1 0> | 285.3 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 67.3 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 285.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 269.0 |
TbScO3 (mp-31119) | <1 1 0> | <1 1 0> | 190.2 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 190.2 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 190.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 269.0 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 269.0 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 285.3 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 285.3 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 285.3 |
Si (mp-149) | <1 0 0> | <1 0 0> | 269.0 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 269.0 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 0> | 95.1 |
MgAl2O4 (mp-3536) | <1 1 1> | <1 1 1> | 116.5 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 269.0 |
C (mp-48) | <1 0 1> | <1 0 0> | 201.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.23 | 0.00 | -0.00 |
0.00 | 2.23 | 0.00 |
-0.00 | 0.00 | 2.23 |
Dielectric Tensor εij (total) |
||
---|---|---|
2.63 | 0.00 | -0.00 |
0.00 | 2.63 | 0.00 |
-0.00 | 0.00 | 2.63 |
Polycrystalline dielectric constant
εpoly∞
2.23
|
Polycrystalline dielectric constant
εpoly
2.63
|
Refractive Index n1.49 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgClO2 (mp-996984) | 0.6152 | 0.253 | 3 |
CCl2O (mp-27727) | 0.4933 | 0.015 | 3 |
BH2N (mp-29475) | 0.6393 | 0.076 | 3 |
BNCl2 (mp-23045) | 0.6713 | 0.240 | 3 |
CN2O (mp-1078789) | 0.6866 | 1.967 | 3 |
H4CN2O (mp-976707) | 0.6127 | 0.023 | 4 |
P2HNF4 (mp-758989) | 0.6217 | 0.067 | 4 |
H4CSN2 (mp-735023) | 0.6826 | 0.010 | 4 |
H4CSN2 (mp-634059) | 0.6301 | 0.054 | 4 |
H6CSN4 (mp-24235) | 0.7058 | 0.167 | 4 |
BCl2 (mp-23316) | 0.5754 | 0.116 | 2 |
BF2 (mp-27864) | 0.4517 | 0.121 | 2 |
NO2 (mp-557865) | 0.4263 | 0.020 | 2 |
NO2 (mp-1771) | 0.2406 | 0.001 | 2 |
NO (mp-1079684) | 0.5482 | 0.888 | 2 |
KCBr(NO2)2 (mp-558178) | 0.7129 | 0.480 | 5 |
Explore more synthesis descriptions for materials of composition NO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: N O |
Final Energy/Atom-6.3058 eV |
Corrected Energy-121.9310 eV
-121.9310 eV = -113.5035 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)