material

AcBr3

ID:

mp-27972

DOI:

10.17188/1202114


Tags: Actinium bromide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.495 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.106 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/m [176]
Hall
-P 6c
Point Group
6/m
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 31578 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WS2 (mp-224) <1 1 1> <0 0 1> 0.008 235.9
ZnO (mp-2133) <0 0 1> <0 0 1> 0.010 176.9
AlN (mp-661) <0 0 1> <0 0 1> 0.010 59.0
Mg (mp-153) <1 0 1> <1 0 1> 0.010 282.7
SiC (mp-8062) <1 1 1> <1 0 0> 0.013 233.6
WS2 (mp-224) <1 1 0> <0 0 1> 0.014 235.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.014 116.8
SiC (mp-7631) <0 0 1> <1 0 0> 0.017 116.8
SiC (mp-11714) <0 0 1> <1 0 0> 0.018 116.8
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.019 350.5
Ag (mp-124) <1 1 0> <1 0 0> 0.020 194.7
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.021 272.6
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.022 272.6
AlN (mp-661) <1 0 1> <1 1 0> 0.025 269.8
BN (mp-984) <0 0 1> <1 0 0> 0.027 233.6
DyScO3 (mp-31120) <0 0 1> <1 0 1> 0.030 282.7
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.030 294.8
GaTe (mp-542812) <1 0 1> <1 0 0> 0.032 194.7
Ni (mp-23) <1 1 0> <1 0 0> 0.034 350.5
ZnO (mp-2133) <1 0 0> <1 0 0> 0.034 350.5
MgO (mp-1265) <1 0 0> <1 1 0> 0.034 269.8
TbScO3 (mp-31119) <0 0 1> <1 0 1> 0.037 282.7
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.041 272.6
Au (mp-81) <1 1 0> <1 0 0> 0.045 194.7
Cu (mp-30) <1 1 0> <0 0 1> 0.051 294.8
C (mp-66) <1 0 0> <1 1 0> 0.055 202.3
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.056 311.5
KCl (mp-23193) <1 0 0> <1 1 0> 0.057 202.3
Ge (mp-32) <1 1 0> <1 0 1> 0.059 141.3
Ni (mp-23) <1 0 0> <1 0 0> 0.061 233.6
GaTe (mp-542812) <1 0 0> <0 0 1> 0.065 176.9
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.065 311.5
GaAs (mp-2534) <1 1 0> <1 0 1> 0.066 141.3
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.066 77.9
CdS (mp-672) <0 0 1> <1 0 0> 0.068 272.6
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.071 311.5
ZnSe (mp-1190) <1 1 0> <1 0 1> 0.075 141.3
C (mp-48) <0 0 1> <1 0 1> 0.080 212.0
WS2 (mp-224) <1 0 0> <1 1 0> 0.081 134.9
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.088 77.9
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.091 155.8
Mg (mp-153) <0 0 1> <1 0 0> 0.093 77.9
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.095 311.5
CdTe (mp-406) <1 1 0> <1 0 0> 0.101 311.5
GaN (mp-804) <1 0 1> <1 0 1> 0.101 282.7
InSb (mp-20012) <1 1 0> <1 0 0> 0.102 311.5
GdScO3 (mp-5690) <0 0 1> <1 0 1> 0.107 282.7
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.124 311.5
CdS (mp-672) <1 1 0> <0 0 1> 0.124 294.8
MgF2 (mp-1249) <0 0 1> <1 1 0> 0.128 67.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
34 13 21 0 0 0
13 34 21 0 0 0
21 21 49 0 0 0
0 0 0 18 0 0
0 0 0 0 18 0
0 0 0 0 0 10
Compliance Tensor Sij (10-12Pa-1)
42.1 -6.7 -15.4 0 0 0
-6.7 42.1 -15.4 0 0 0
-15.4 -15.4 34.1 0 0 0
0 0 0 55.5 0 0
0 0 0 0 55.5 0
0 0 0 0 0 97.6
Shear Modulus GV
13 GPa
Bulk Modulus KV
25 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
23 GPa
Shear Modulus GVRH
13 GPa
Bulk Modulus KVRH
24 GPa
Elastic Anisotropy
0.62
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ScSiPt2 (mp-13572) 0.6997 0.000 3
ErGePd2 (mp-20819) 0.7364 0.000 3
NdCl3 (mp-23183) 0.1008 0.000 2
UCl3 (mp-23208) 0.0860 0.000 2
PrCl3 (mp-23211) 0.0849 0.000 2
LaCl3 (mp-22896) 0.0977 0.000 2
PuCl3 (mp-22918) 0.0902 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ac Br
Final Energy/Atom
-4.3520 eV
Corrected Energy
-38.0202 eV
Uncorrected energy = -34.8162 eV Composition-based energy adjustment (-0.534 eV/atom x 6.0 atoms) = -3.2040 eV Corrected energy = -38.0202 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 31578
Submitted by
User remarks:
  • Actinium bromide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)