Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.908 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.058 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSnSO4 + S8O + SnO2 |
Band Gap3.508 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP421c [114] |
HallP 4 2n |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 0 1> | 253.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 126.8 |
TePb (mp-19717) | <1 1 1> | <1 1 0> | 144.4 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 126.8 |
TeO2 (mp-2125) | <1 1 0> | <1 1 1> | 192.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 126.8 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 126.8 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 126.8 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 126.8 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 126.8 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 144.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 253.6 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 204.2 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 102.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 126.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 126.8 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 253.6 |
WS2 (mp-224) | <1 1 0> | <1 0 1> | 162.8 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 126.8 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 253.6 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 253.6 |
YAlO3 (mp-3792) | <0 1 1> | <1 1 0> | 144.4 |
YAlO3 (mp-3792) | <1 0 1> | <1 1 0> | 144.4 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 126.8 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 126.8 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 126.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg2SO4 (mp-7461) | 0.3705 | 0.000 | 3 |
Hg2SeO4 (mp-7462) | 0.4047 | 0.016 | 3 |
Pb3SO6 (mp-559143) | 0.4694 | 0.004 | 3 |
SnSO4 (mp-645740) | 0.4659 | 0.024 | 3 |
K4CO4 (mp-550895) | 0.4898 | 0.221 | 3 |
NaLiSO4 (mp-6783) | 0.5646 | 0.000 | 4 |
Sn3PO4F3 (mp-546757) | 0.5431 | 0.000 | 4 |
H4NClO4 (mp-698084) | 0.5849 | 0.350 | 4 |
LiSnPO4 (mp-757590) | 0.5954 | 0.060 | 4 |
H2Pb4SO8 (mp-697676) | 0.4705 | 0.001 | 4 |
H34C19 (mp-866659) | 0.6411 | 0.060 | 2 |
H34C19 (mp-30168) | 0.6628 | 0.055 | 2 |
GaBr2 (mp-650841) | 0.6711 | 0.011 | 2 |
PBr7 (mp-647343) | 0.6750 | 0.000 | 2 |
VCl4 (mp-570763) | 0.6784 | 0.004 | 2 |
TlZnSClO4 (mp-23146) | 0.6116 | 0.000 | 5 |
KBiS(ClO2)2 (mp-23645) | 0.6107 | 0.000 | 5 |
PH4N(OF)2 (mp-706976) | 0.6286 | 0.000 | 5 |
RbZnSClO4 (mp-559540) | 0.6268 | 0.000 | 5 |
RbSbS(O2F)2 (mp-554732) | 0.5748 | 0.000 | 5 |
SiBHC3NCl2 (mp-698440) | 0.7299 | 0.908 | 6 |
BH11C4NClF4 (mp-559235) | 0.5944 | 0.113 | 6 |
BH11C4BrNF4 (mp-554318) | 0.6211 | 0.111 | 6 |
KSn2H36C12(Se2N)3 (mp-708999) | 0.7055 | 0.088 | 6 |
FeGe4H24C8(S5N)2 (mp-736330) | 0.7467 | 0.083 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d S O |
Final Energy/Atom-5.9933 eV |
Corrected Energy-415.0758 eV
Uncorrected energy = -383.5718 eV
Composition-based energy adjustment (-0.503 eV/atom x 8.0 atoms) = -4.0240 eV
Composition-based energy adjustment (-0.687 eV/atom x 40.0 atoms) = -27.4800 eV
Corrected energy = -415.0758 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)