Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.499 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.401 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPna21 [33] |
HallP 2c 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 277.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 281.3 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 199.9 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 55.5 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 196.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 120.6 |
AlN (mp-661) | <1 1 0> | <0 1 1> | 55.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 114.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 166.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 333.2 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 333.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 120.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 281.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 120.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 321.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 153.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 55.5 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 321.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 191.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 160.7 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 327.6 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 230.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 120.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 306.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 160.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 277.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 160.7 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 319.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 191.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 212.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 268.1 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 307.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 344.6 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 191.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 153.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 268.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 212.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 241.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 327.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 153.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 229.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 268.1 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 333.1 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 166.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 160.7 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 160.7 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 262.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 212.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 268.1 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 199.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.04901 |
0.05028 | -0.41206 | -0.05475 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.10252 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.41871 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.15 | 0.00 | 0.00 |
0.00 | 2.19 | 0.00 |
0.00 | 0.00 | 2.22 |
Dielectric Tensor εij (total) |
||
---|---|---|
3.20 | 0.00 | 0.00 |
0.00 | 3.47 | 0.00 |
0.00 | 0.00 | 9.04 |
Polycrystalline dielectric constant
εpoly∞
2.19
|
Polycrystalline dielectric constant
εpoly
5.24
|
Refractive Index n1.48 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TlGeF3 (mp-998712) | 0.5827 | 0.028 | 3 |
NaClO3 (mp-630949) | 0.5966 | 0.615 | 3 |
SeOF2 (mp-27367) | 0.5096 | 0.000 | 3 |
PHF2 (mp-24064) | 0.3444 | 0.115 | 3 |
SbNO (mp-758558) | 0.5846 | 0.036 | 3 |
BaHClO (mp-24565) | 0.6243 | 0.000 | 4 |
AsCl3 (mp-23280) | 0.3288 | 0.000 | 2 |
AsBr3 (mp-23317) | 0.3917 | 0.000 | 2 |
SbBr3 (mp-27399) | 0.4053 | 0.000 | 2 |
SbBr3 (mp-570005) | 0.4130 | 0.000 | 2 |
SbCl3 (mp-22872) | 0.4069 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: As F |
Final Energy/Atom-4.7289 eV |
Corrected Energy-75.6626 eV
-75.6626 eV = -75.6626 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)