@article{Ruehl1982, author = "Ruehl, R. and Jeitschko, W.", title = "Preparation and Structure of Technetium Triphosphide and Rhenium Triphosphide, Isotypic Polyphosphides with Metal Chains", journal = "Acta Crystallographica B (24,1968-38,1982)", year = "1982", volume = "38", pages = "2784-2788", ASTM_id = "ACBCAR" }