material

TmCl3

ID:

mp-28044

DOI:

10.17188/1202173


Tags: Thulium chloride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.691 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.96 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
5.023 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3c [167]
Hall
-R 3 2"c
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 35398 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbSe (mp-2201) <1 1 1> <0 0 1> 0.000 268.7
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.000 38.4
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.000 38.4
GaSb (mp-1156) <1 1 1> <0 0 1> 0.001 268.7
LiF (mp-1138) <1 1 1> <0 0 1> 0.001 115.2
BN (mp-984) <0 0 1> <0 0 1> 0.001 38.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.001 345.5
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.002 115.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.002 115.2
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.002 115.2
CdSe (mp-2691) <1 1 1> <0 0 1> 0.002 268.7
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.002 153.6
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.003 153.6
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.006 153.6
C (mp-66) <1 1 1> <0 0 1> 0.008 153.6
Mg (mp-153) <0 0 1> <0 0 1> 0.008 115.2
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.011 191.9
MgF2 (mp-1249) <1 1 1> <1 0 0> 0.012 120.1
GaN (mp-804) <0 0 1> <0 0 1> 0.012 115.2
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.013 153.6
Si (mp-149) <1 1 1> <0 0 1> 0.014 153.6
CdTe (mp-406) <1 0 0> <0 0 1> 0.015 307.1
InSb (mp-20012) <1 0 0> <0 0 1> 0.016 307.1
GaSe (mp-1943) <0 0 1> <0 0 1> 0.018 38.4
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.019 268.7
LiF (mp-1138) <1 0 0> <0 0 1> 0.020 268.7
InAs (mp-20305) <1 1 1> <0 0 1> 0.022 268.7
TiO2 (mp-390) <0 0 1> <0 0 1> 0.023 307.1
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.025 191.9
Ge (mp-32) <1 0 0> <0 0 1> 0.027 268.7
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.031 268.7
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.033 126.1
Al (mp-134) <1 1 1> <0 0 1> 0.034 115.2
GaAs (mp-2534) <1 0 0> <0 0 1> 0.038 268.7
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.039 307.1
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.041 268.7
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.042 191.9
TePb (mp-19717) <1 0 0> <0 0 1> 0.043 307.1
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.047 268.7
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.050 115.2
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.054 268.7
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.058 230.3
Ni (mp-23) <1 1 0> <0 0 1> 0.064 345.5
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.066 191.9
GaP (mp-2490) <1 1 1> <0 0 1> 0.066 153.6
BN (mp-984) <1 1 0> <0 0 1> 0.069 268.7
CdTe (mp-406) <1 1 0> <0 0 1> 0.073 307.1
InSb (mp-20012) <1 1 0> <0 0 1> 0.076 307.1
Ni (mp-23) <1 1 1> <0 0 1> 0.079 153.6
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.080 268.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
26 -5 10 -9 0 0
-5 26 10 9 0 0
10 10 39 0 0 0
-9 9 0 20 0 0
0 0 0 0 20 -9
0 0 0 0 -9 15
Compliance Tensor Sij (10-12Pa-1)
52 9.2 -16.1 18.4 0 0
9.2 52 -16.1 -18.4 0 0
-16.1 -16.1 33.8 0 0 0
18.4 -18.4 0 65.5 0 0
0 0 0 0 65.5 36.9
0 0 0 0 36.9 85.6
Shear Modulus GV
16 GPa
Bulk Modulus KV
14 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
11 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
12 GPa
Elastic Anisotropy
2.26
Poisson's Ratio
0.09

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnPtF6 (mp-8256) 0.1004 0.000 3
NiPbF6 (mp-559408) 0.1023 0.000 3
NiPtF6 (mp-558838) 0.0807 0.000 3
NiPtF6 (mp-612185) 0.0921 0.000 3
NiPbF6 (mp-611642) 0.1056 0.000 3
Cs2LiAl3F12 (mp-13634) 0.6939 0.000 4
NiF3 (mp-561428) 0.1514 0.000 2
MoF3 (mp-557539) 0.1586 0.000 2
PdF3 (mp-13679) 0.0438 0.000 2
TeO3 (mp-2552) 0.1045 0.020 2
RuF3 (mp-7570) 0.0890 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Tm_3 Cl
Final Energy/Atom
-4.7507 eV
Corrected Energy
-38.0056 eV
-38.0056 eV = -38.0056 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 35398
Submitted by
User remarks:
  • Thulium chloride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)