Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.705 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.942 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 134.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 134.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 311.1 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 155.5 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 77.8 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 134.8 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 233.3 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 155.5 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 311.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 77.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 134.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 233.3 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 137.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 311.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 77.8 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 0> | 192.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 311.1 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 192.2 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 192.2 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 192.2 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 77.8 |
CdSe (mp-2691) | <1 1 1> | <0 1 0> | 134.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 137.0 |
BN (mp-984) | <1 0 0> | <1 1 0> | 192.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 134.8 |
BN (mp-984) | <1 1 1> | <0 1 0> | 134.8 |
C (mp-48) | <0 0 1> | <1 0 0> | 137.0 |
C (mp-48) | <1 0 0> | <1 1 0> | 192.2 |
C (mp-48) | <1 1 0> | <0 1 0> | 134.8 |
C (mp-48) | <1 1 1> | <0 1 0> | 134.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 233.3 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 134.8 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 155.5 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 155.5 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 192.2 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 233.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 233.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 311.1 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 155.6 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 77.8 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 233.3 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 311.1 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 233.3 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 233.3 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 311.1 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 77.8 |
GaSb (mp-1156) | <1 1 1> | <0 1 0> | 134.8 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 311.1 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 155.5 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 311.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -0.18449 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.72258 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.20645 |
Piezoelectric Modulus ‖eij‖max0.72258 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.72 | 0.00 | 0.00 |
0.00 | 6.51 | 0.00 |
0.00 | 0.00 | 6.64 |
Dielectric Tensor εij (total) |
||
---|---|---|
34.20 | 0.00 | 0.00 |
0.00 | 33.89 | 0.00 |
0.00 | 0.00 | 15.17 |
Polycrystalline dielectric constant
εpoly∞
6.62
|
Polycrystalline dielectric constant
εpoly
27.75
|
Refractive Index n2.57 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na8Cu2O7 (mp-779159) | 0.4849 | 0.126 | 3 |
Ca7GeN6 (mp-570555) | 0.4656 | 0.014 | 3 |
Na7In3Se8 (mp-541689) | 0.4663 | 0.000 | 3 |
Na4TiSe4 (mp-505798) | 0.4690 | 0.000 | 3 |
Na3GaS3 (mp-561130) | 0.4923 | 0.000 | 3 |
CuBiPbS3 (mp-624191) | 0.5853 | 0.009 | 4 |
CsK4TlO4 (mp-562074) | 0.6012 | 0.000 | 4 |
Na3CuSnSe4 (mp-623030) | 0.4620 | 0.017 | 4 |
Na8Li9(FeO4)4 (mp-771278) | 0.5756 | 0.034 | 4 |
Sm3MnAlS7 (mp-867965) | 0.6028 | 0.089 | 4 |
In4Te3 (mp-617281) | 0.6957 | 0.000 | 2 |
MgSi2 (mp-1073530) | 0.6817 | 0.234 | 2 |
MgSi2 (mp-1073539) | 0.7095 | 0.182 | 2 |
Mg5Si9 (mp-1075724) | 0.7041 | 0.253 | 2 |
Tl4S3 (mp-2753) | 0.6741 | 0.009 | 2 |
Li4Ca2Mg(SiN3)2 (mp-1020016) | 0.7459 | 0.000 | 5 |
LiCaMgSiN3 (mp-1020108) | 0.6890 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Sn_d Te |
Final Energy/Atom-3.1286 eV |
Corrected Energy-119.3826 eV
Uncorrected energy = -112.6306 eV
Composition-based energy adjustment (-0.422 eV/atom x 16.0 atoms) = -6.7520 eV
Corrected energy = -119.3826 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)