material

Rb2PtI6

ID:

mp-28110

DOI:

10.17188/1202227


Tags: Rubidium hexaiodoplatinate

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.786 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.88 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.513 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ge (mp-32) <1 0 0> <1 0 0> 0.000 133.0
Ge (mp-32) <1 1 0> <1 1 0> 0.000 188.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.001 133.0
LiF (mp-1138) <1 1 0> <1 1 0> 0.001 188.1
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.002 133.0
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.002 188.1
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.002 188.1
GaAs (mp-2534) <1 0 0> <1 0 0> 0.005 133.0
GaAs (mp-2534) <1 1 0> <1 1 0> 0.005 188.1
InSb (mp-20012) <1 1 0> <1 1 0> 0.009 188.1
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.009 188.1
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.010 133.0
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.010 188.1
CdTe (mp-406) <1 1 0> <1 1 0> 0.012 188.1
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.018 266.0
Si (mp-149) <1 0 0> <1 0 0> 0.020 266.0
ZnO (mp-2133) <0 0 1> <1 1 0> 0.026 188.1
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.045 188.1
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.046 266.0
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.058 188.1
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.078 188.1
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.082 133.0
TePb (mp-19717) <1 1 0> <1 1 0> 0.111 188.1
Mg (mp-153) <1 0 1> <1 1 0> 0.163 188.1
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.177 133.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
15 7 7 0 -0 -0
7 15 7 -0 0 -0
7 7 15 0 -0 0
0 -0 0 5 0 0
-0 0 -0 0 5 0
-0 -0 0 0 0 5
Compliance Tensor Sij (10-12Pa-1)
91.9 -28.1 -28.1 0 0 0
-28.1 91.9 -28.1 0 0 0
-28.1 -28.1 91.9 0 0 0
0 0 0 194 0 0
0 0 0 0 194 0
0 0 0 0 0 194
Shear Modulus GV
5 GPa
Bulk Modulus KV
9 GPa
Shear Modulus GR
5 GPa
Bulk Modulus KR
9 GPa
Shear Modulus GVRH
5 GPa
Bulk Modulus KVRH
9 GPa
Elastic Anisotropy
0.05
Poisson's Ratio
0.28

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.15 0.00 0.00
0.00 5.15 0.00
0.00 0.00 5.15
Dielectric Tensor εij (total)
10.95 -0.00 0.00
-0.00 10.95 0.00
0.00 0.00 10.95
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.15
Polycrystalline dielectric constant εpoly
(total)
10.95
Refractive Index n
2.27
Potentially ferroelectric?
True

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
28
U Values
--
Pseudopotentials
VASP PAW: Rb_sv I Pt
Final Energy/Atom
-2.6858 eV
Corrected Energy
-24.1722 eV
-24.1722 eV = -24.1722 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 37191

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)