Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.709 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.201 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYbO + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIa3 [206] |
Hall-I 2b 2c 3 |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 162.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 114.6 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 162.1 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 198.5 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 198.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 198.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 162.1 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 162.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 198.5 |
Al (mp-134) | <1 1 1> | <1 1 1> | 198.5 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 162.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 229.2 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 114.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 162.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 198.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 114.6 |
C (mp-66) | <1 1 1> | <1 1 1> | 198.5 |
C (mp-66) | <1 1 0> | <1 1 0> | 162.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 229.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 229.2 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 114.6 |
PbSe (mp-2201) | <1 1 1> | <1 1 1> | 198.5 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 162.1 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 229.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 229.2 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 162.1 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 198.5 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 114.6 |
CaCO3 (mp-3953) | <0 0 1> | <1 1 1> | 198.5 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 162.1 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 114.6 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 114.6 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 162.1 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 114.6 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 162.1 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 162.1 |
GaSb (mp-1156) | <1 1 1> | <1 1 1> | 198.5 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 162.1 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 198.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y7HoO12 (mp-762307) | 0.1887 | 0.001 | 3 |
Gd5Y3O12 (mp-752459) | 0.1874 | 0.000 | 3 |
Dy3Y5O12 (mp-752458) | 0.1892 | 0.000 | 3 |
Dy11Y5O24 (mp-766279) | 0.1815 | 0.000 | 3 |
Sm27Y5O48 (mp-861145) | 0.1820 | 0.020 | 3 |
Li2VSi3O8 (mp-767616) | 0.6104 | 0.092 | 4 |
CaLa2BiO6 (mvc-15176) | 0.5966 | 0.078 | 4 |
Mg2VWO6 (mvc-5881) | 0.6268 | 0.018 | 4 |
Mg2TiWO6 (mvc-5939) | 0.6184 | 0.128 | 4 |
InNi2SbO6 (mp-1078367) | 0.5664 | 0.000 | 4 |
Pu2O3 (mp-637224) | 0.1268 | 0.000 | 2 |
Pm2O3 (mp-553921) | 0.1372 | 0.000 | 2 |
Nd2O3 (mp-1045) | 0.1255 | 0.000 | 2 |
Pr2O3 (mp-16705) | 0.1149 | 0.000 | 2 |
La2O3 (mp-2292) | 0.0691 | 0.000 | 2 |
Explore more synthesis descriptions for materials of composition Yb2O3.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 O |
Final Energy/Atom-5.8718 eV |
Corrected Energy-251.7285 eV
-251.7285 eV = -234.8736 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)