Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.154 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb3Sb2Br9 |
Band Gap1.905 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 224.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 224.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 236.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 280.6 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 290.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 96.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 136.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 56.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 168.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 224.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 224.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 157.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 236.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 193.3 |
Ni (mp-23) | <1 0 0> | <1 1 1> | 147.4 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 280.6 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 224.5 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 96.7 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 168.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 96.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 136.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 56.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 96.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 136.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 314.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 224.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 236.1 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 157.4 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 1> | 193.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 168.4 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 236.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 290.0 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 224.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 224.5 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 290.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 314.8 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 168.4 |
WS2 (mp-224) | <1 0 0> | <1 1 0> | 136.3 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 224.5 |
WS2 (mp-224) | <1 1 1> | <0 0 1> | 224.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 224.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 168.4 |
BN (mp-984) | <1 0 0> | <1 0 1> | 96.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 224.5 |
BN (mp-984) | <1 1 1> | <1 0 0> | 236.1 |
C (mp-48) | <1 0 1> | <0 0 1> | 336.8 |
C (mp-48) | <1 1 1> | <1 0 0> | 236.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 168.4 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 224.5 |
NaCl (mp-22862) | <1 0 0> | <1 0 1> | 96.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs3Bi2Br9 (mp-27544) | 0.0660 | 0.000 | 3 |
Cs3Sb2Cl9 (mp-27629) | 0.1738 | 0.000 | 3 |
Cs3Bi2Br9 (mp-680674) | 0.1474 | 0.001 | 3 |
Cs3Sb2Br9 (mp-579560) | 0.0943 | 0.000 | 3 |
Cs3Sb2I9 (mp-541014) | 0.0526 | 0.005 | 3 |
Ba8Nb6CoO24 (mp-640790) | 0.5818 | 0.018 | 4 |
K4BaU3O12 (mp-19965) | 0.7212 | 0.036 | 4 |
Sr4Re2NiO12 (mp-32309) | 0.3813 | 0.011 | 4 |
Ba5Li2(WO5)3 (mp-566745) | 0.7355 | 0.000 | 4 |
Ba6Lu2(WO6)3 (mp-19673) | 0.5474 | 0.000 | 4 |
K6Ba2CaU6O24 (mp-691065) | 0.5008 | 0.023 | 5 |
Ba4La2Ti3Nb2O18 (mp-684815) | 0.6326 | 0.042 | 5 |
Ba3LaIn(WO6)2 (mp-705477) | 0.5025 | 0.066 | 5 |
Ba2La2Zn(WO6)2 (mp-41236) | 0.5429 | 0.108 | 5 |
Ba2La2Mn(WO6)2 (mp-566048) | 0.5863 | 0.074 | 5 |
Ba3LaZnReWO12 (mp-705508) | 0.3351 | 0.057 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Sb Br |
Final Energy/Atom-3.0063 eV |
Corrected Energy-46.8936 eV
Uncorrected energy = -42.0876 eV
Composition-based energy adjustment (-0.534 eV/atom x 9.0 atoms) = -4.8060 eV
Corrected energy = -46.8936 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)