Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.665 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.527 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P1 [2]
Hall
-P 1
Point Group
1
Crystal System
triclinic

Electronic Structure

Topological data for ICSD ID 35498 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ga2O3 (mp-886) <1 1 -1> <1 0 -1> 0.002 80.5
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.003 309.8
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.003 242.2
BN (mp-984) <0 0 1> <0 0 1> 0.005 201.8
SiC (mp-11714) <1 0 0> <0 0 1> 0.010 282.6
C (mp-48) <1 1 1> <0 0 1> 0.012 201.8
LiAlO2 (mp-3427) <1 1 0> <0 1 1> 0.012 93.3
Ga2O3 (mp-886) <1 1 0> <1 -1 1> 0.012 294.3
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.015 161.5
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.018 232.4
BaF2 (mp-1029) <1 1 0> <0 1 1> 0.019 280.0
GaSe (mp-1943) <0 0 1> <0 0 1> 0.022 242.2
Mg (mp-153) <0 0 1> <0 1 1> 0.024 280.0
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.026 282.6
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.029 150.1
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.029 232.4
MoS2 (mp-1434) <0 0 1> <0 1 1> 0.029 280.0
WS2 (mp-224) <0 0 1> <0 1 1> 0.029 280.0
GaSe (mp-1943) <1 1 0> <1 0 0> 0.030 232.4
LaAlO3 (mp-2920) <0 0 1> <1 0 1> 0.031 281.1
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.031 322.9
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.035 309.8
GaN (mp-804) <0 0 1> <0 0 1> 0.038 282.6
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.038 282.6
LaF3 (mp-905) <1 1 0> <0 0 1> 0.038 282.6
ZnO (mp-2133) <0 0 1> <1 0 -1> 0.038 241.5
SiC (mp-8062) <1 0 0> <0 0 1> 0.040 322.9
C (mp-66) <1 0 0> <0 0 1> 0.041 201.8
BaF2 (mp-1029) <1 0 0> <0 1 1> 0.041 280.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.042 282.6
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.042 282.6
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.043 282.6
Cu (mp-30) <1 1 0> <0 0 1> 0.044 201.8
LiAlO2 (mp-3427) <1 0 0> <0 1 0> 0.044 300.2
AlN (mp-661) <1 0 1> <0 0 1> 0.045 282.6
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.045 242.2
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.045 242.2
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.046 282.6
C (mp-48) <0 0 1> <0 0 1> 0.046 282.6
BN (mp-984) <1 1 1> <1 1 -1> 0.047 236.7
MgO (mp-1265) <1 1 0> <0 0 1> 0.047 282.6
MgO (mp-1265) <1 0 0> <1 0 -1> 0.048 161.0
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.051 309.8
SiC (mp-7631) <1 0 1> <0 0 1> 0.051 242.2
MgF2 (mp-1249) <1 1 0> <0 1 -1> 0.051 305.0
ZnO (mp-2133) <1 0 1> <0 0 1> 0.053 40.4
ZnO (mp-2133) <1 1 1> <0 0 1> 0.053 161.5
ZnO (mp-2133) <1 1 0> <1 -1 0> 0.056 91.1
CdS (mp-672) <1 0 0> <0 0 1> 0.057 282.6
Ni (mp-23) <1 0 0> <0 0 1> 0.062 201.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
55 4 8 -1 2 0
4 16 6 -1 -2 0
8 6 25 -0 0 0
-1 -1 -0 3 0 -2
2 -2 0 0 6 -0
0 0 0 -2 -0 3
Compliance Tensor Sij (10-12Pa-1)
19.3 -2.9 -5.5 2.1 -5.8 -1.6
-2.9 73.6 -15.8 42.9 27 30.2
-5.5 -15.8 45.6 -8.2 -6.5 -8.6
2.1 42.9 -8.2 904.6 35.4 634.1
-5.8 27 -6.5 35.4 176.3 47.3
-1.6 30.2 -8.6 634.1 47.3 754.4
Shear Modulus GV
8 GPa
Bulk Modulus KV
15 GPa
Shear Modulus GR
2 GPa
Bulk Modulus KR
11 GPa
Shear Modulus GVRH
5 GPa
Bulk Modulus KVRH
13 GPa
Elastic Anisotropy
11.10
Poisson's Ratio
0.33

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
7.93 0.15 0.66
0.15 7.10 -0.03
0.66 -0.03 11.48
Dielectric Tensor εij (total)
21.04 0.34 10.10
0.34 13.36 -4.24
10.10 -4.24 147.06
Polycrystalline dielectric constant εpoly
(electronic contribution)
8.83
Polycrystalline dielectric constant εpoly
(total)
60.49
Refractive Index n
2.97
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba2Bi2O5 (mp-28670) 0.6583 0.000 3
TlAsSe2 (mp-30236) 0.6056 0.000 3
KSbSe2 (mp-542642) 0.3391 0.014 3
RbSbS2 (mp-10621) 0.3708 0.000 3
Na2Sb4O7 (mp-30972) 0.6401 0.000 3
RbNaTiO3 (mp-556185) 0.7338 0.000 4
CsNaTiO3 (mp-560791) 0.7475 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Tl_d Sb S
Final Energy/Atom
-4.0244 eV
Corrected Energy
-69.6979 eV
-69.6979 eV = -64.3902 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 650825
  • 35498
Submitted by
User remarks:
  • Thallium antimony sulfide (1/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)