Final Magnetic Moment0.018 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.297 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.120 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaPrO2 + Na2O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 226.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 139.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 278.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 301.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 301.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 112.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 208.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 278.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 278.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 112.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 208.9 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 139.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 278.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 301.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 69.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 112.7 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 205.3 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 150.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 69.6 |
Al (mp-134) | <1 1 1> | <1 0 0> | 112.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 69.6 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 113.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 226.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 208.9 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 208.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 208.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 208.9 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 278.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 301.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 226.2 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 0 1> | 208.9 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 208.9 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 278.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 69.6 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 208.9 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 112.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 278.5 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 112.7 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 278.5 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 226.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 112.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 208.9 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 208.9 |
C (mp-48) | <0 0 1> | <0 1 0> | 301.7 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 278.5 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 112.7 |
WSe2 (mp-1821) | <1 0 0> | <1 0 1> | 149.5 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 139.3 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 278.5 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 226.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiCoO2 (mp-868388) | 0.1581 | 0.090 | 3 |
LiVO2 (mp-764772) | 0.1605 | 0.237 | 3 |
Li7Ni5O12 (mp-773266) | 0.1583 | 0.007 | 3 |
Li2CrO3 (mp-769772) | 0.1518 | 0.020 | 3 |
Li2CrS3 (mp-756176) | 0.1526 | 0.169 | 3 |
Li4TiCrO6 (mp-769687) | 0.1180 | 0.068 | 4 |
Li24Ti7Cr5O36 (mp-771300) | 0.1200 | 0.104 | 4 |
Li24Ti7Cr5O36 (mp-771285) | 0.1173 | 0.128 | 4 |
Li24Ti7Cr5O36 (mp-771284) | 0.1203 | 0.177 | 4 |
Li24TiCr11O36 (mp-777927) | 0.1196 | 0.083 | 4 |
Te2Au (mp-1662) | 0.3459 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3691 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.3623 | 0.009 | 2 |
Ga2Te3 (mp-1070116) | 0.4101 | 0.334 | 2 |
Te2Au (mp-567525) | 0.3517 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.3699 | 0.139 | 5 |
Na (mp-999501) | 0.6320 | 0.114 | 1 |
Sb (mp-632286) | 0.4901 | 0.059 | 1 |
Bi (mp-23152) | 0.6214 | 0.000 | 1 |
Te (mp-570459) | 0.4788 | 0.044 | 1 |
Te (mp-105) | 0.5792 | 0.047 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Pr_3 O |
Final Energy/Atom-5.6538 eV |
Corrected Energy-144.1189 eV
-144.1189 eV = -135.6914 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)