Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.618 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.77 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToThSi2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 204.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 204.0 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 248.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 34.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 153.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 238.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 248.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 255.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 221.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 289.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 356.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 248.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 289.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 153.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 170.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 253.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 169.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 272.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 170.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 85.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 119.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 85.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 187.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 299.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 272.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 85.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 289.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 299.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 85.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 136.0 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 186.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 169.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 306.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 153.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 34.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 17.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 221.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 85.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 17.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 239.2 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 310.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 289.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 179.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 204.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 323.0 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 186.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SmAlGe (mp-3077) | 0.0424 | 0.000 | 3 |
GdAlGe (mp-1025108) | 0.0458 | 0.071 | 3 |
CeSiNi (mp-20710) | 0.0438 | 0.000 | 3 |
SmAlSi (mp-12804) | 0.0387 | 0.000 | 3 |
CeSiNi (mp-1072275) | 0.0473 | 0.000 | 3 |
GdSi2 (mp-1076954) | 0.0167 | 0.000 | 2 |
PuSi2 (mp-21105) | 0.0120 | 0.590 | 2 |
CeSi2 (mp-1898) | 0.0447 | 0.000 | 2 |
SmSi2 (mp-13955) | 0.0098 | 0.000 | 2 |
PuSi2 (mp-1077579) | 0.0263 | 0.590 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th Si |
Final Energy/Atom-6.7052 eV |
Corrected Energy-40.2310 eV
-40.2310 eV = -40.2310 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)