material

DyCl3

ID:

mp-28448

DOI:

10.17188/1202552


Tags: Dysprosium chloride

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.713 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.90 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.900 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-7631) <1 0 0> <0 1 1> 0.002 236.4
TiO2 (mp-390) <1 0 0> <0 0 1> 0.003 148.0
Te2W (mp-22693) <1 0 0> <0 1 1> 0.004 295.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.004 148.0
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.004 345.3
LaAlO3 (mp-2920) <1 1 0> <1 0 1> 0.005 121.8
TiO2 (mp-390) <1 0 1> <0 1 1> 0.008 118.2
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.010 345.3
CdTe (mp-406) <1 1 0> <1 0 1> 0.010 121.8
Al (mp-134) <1 1 0> <0 0 1> 0.011 345.3
InSb (mp-20012) <1 1 0> <1 0 1> 0.011 121.8
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.011 345.3
InSb (mp-20012) <1 0 0> <0 0 1> 0.011 345.3
CdTe (mp-406) <1 0 0> <0 0 1> 0.012 345.3
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.014 222.6
CaCO3 (mp-3953) <1 0 0> <0 1 0> 0.019 260.3
TiO2 (mp-390) <0 0 1> <0 1 1> 0.023 59.1
Te2W (mp-22693) <0 0 1> <1 0 1> 0.026 243.5
KTaO3 (mp-3614) <1 1 0> <0 0 1> 0.028 246.6
WSe2 (mp-1821) <1 1 1> <0 1 0> 0.031 260.3
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.032 345.3
LiAlO2 (mp-3427) <1 0 1> <0 0 1> 0.034 345.3
C (mp-48) <0 0 1> <0 0 1> 0.035 148.0
LiNbO3 (mp-3731) <1 0 0> <0 1 0> 0.036 292.8
GaSe (mp-1943) <1 0 0> <0 0 1> 0.036 197.3
C (mp-66) <1 1 1> <0 0 1> 0.037 345.3
LiTaO3 (mp-3666) <1 0 0> <0 1 0> 0.040 292.8
TePb (mp-19717) <1 1 0> <1 0 1> 0.042 121.8
WSe2 (mp-1821) <1 1 0> <0 1 0> 0.044 260.3
GaN (mp-804) <1 0 1> <0 1 0> 0.045 325.4
AlN (mp-661) <1 0 0> <0 1 1> 0.046 236.4
LiF (mp-1138) <1 1 0> <0 0 1> 0.048 345.3
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.051 121.8
MgO (mp-1265) <1 0 0> <0 1 1> 0.058 236.4
Cu (mp-30) <1 0 0> <0 0 1> 0.059 345.3
LiGaO2 (mp-5854) <0 1 1> <0 1 0> 0.062 130.1
CdWO4 (mp-19387) <1 1 0> <0 1 0> 0.063 162.7
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.063 345.3
KCl (mp-23193) <1 0 0> <0 0 1> 0.072 246.6
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.072 231.9
Cu (mp-30) <1 1 0> <0 0 1> 0.075 246.6
MoSe2 (mp-1634) <1 1 0> <0 1 1> 0.077 177.3
TePb (mp-19717) <1 0 0> <0 0 1> 0.087 345.3
LiF (mp-1138) <1 1 1> <0 1 0> 0.089 260.3
PbS (mp-21276) <1 0 0> <0 1 0> 0.090 292.8
SiC (mp-7631) <0 0 1> <0 1 0> 0.106 227.8
C (mp-66) <1 0 0> <0 1 0> 0.108 357.9
SiO2 (mp-6930) <1 0 0> <0 1 0> 0.108 195.2
AlN (mp-661) <0 0 1> <0 1 0> 0.109 162.7
SiC (mp-11714) <0 0 1> <0 1 0> 0.113 227.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
56 1 27 0 0 0
1 3 2 0 0 0
27 2 77 0 0 0
0 0 0 1 0 0
0 0 0 0 19 0
0 0 0 0 0 0
Compliance Tensor Sij (10-12Pa-1)
21.6 -3.4 -7.6 0 0 0
-3.4 367.2 -6.4 0 0 0
-7.6 -6.4 15.9 0 0 0
0 0 0 1245.6 0 0
0 0 0 0 52.6 0
0 0 0 0 0 2769.7
Shear Modulus GV
11 GPa
Bulk Modulus KV
22 GPa
Shear Modulus GR
1 GPa
Bulk Modulus KR
3 GPa
Shear Modulus GVRH
6 GPa
Bulk Modulus KVRH
12 GPa
Elastic Anisotropy
53.28
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CaThBr6 (mp-29015) 0.4632 0.053 3
SrThBr6 (mp-29016) 0.5875 0.045 3
BaThBr6 (mp-570615) 0.5795 0.061 3
TbCl3 (mp-23293) 0.1640 0.004 2
PuBr3 (mp-27974) 0.1723 0.000 2
NdBr3 (mp-27975) 0.1850 0.000 2
SmBr3 (mp-27976) 0.1698 0.000 2
NpBr3 (mp-567519) 0.2459 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Dy_3 Cl
Final Energy/Atom
-4.7903 eV
Corrected Energy
-42.0067 eV
Uncorrected energy = -38.3227 eV Composition-based energy adjustment (-0.614 eV/atom x 6.0 atoms) = -3.6840 eV Corrected energy = -42.0067 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 40064
Submitted by
User remarks:
  • Dysprosium chloride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)