Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.899 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.56 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.544 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nbm [125] |
HallP 4 2 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 287.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 293.8 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 287.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 287.4 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 249.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 151.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 302.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 75.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 176.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 95.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 302.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 75.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 302.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 287.4 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 249.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 151.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 176.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 249.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 293.8 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 293.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 176.3 |
GaSe (mp-1943) | <1 1 0> | <1 0 0> | 117.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 176.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 176.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 1> | 287.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 176.3 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 249.3 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 235.1 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 302.7 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 75.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 293.8 |
MgO (mp-1265) | <1 1 1> | <1 1 0> | 249.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 176.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 58.8 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 58.8 |
C (mp-66) | <1 0 0> | <1 0 1> | 191.6 |
C (mp-66) | <1 1 0> | <1 0 0> | 293.8 |
C (mp-66) | <1 1 1> | <1 0 0> | 176.3 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 293.8 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 287.4 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 227.0 |
PbS (mp-21276) | <1 0 0> | <1 0 1> | 287.4 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 151.3 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 302.7 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 293.8 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 176.3 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 249.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 75.7 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 235.1 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 151.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
7.61 | 0.00 | 0.00 |
0.00 | 6.29 | 0.00 |
0.00 | 0.00 | 6.29 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.82 | 0.00 | 0.00 |
0.00 | 9.86 | 0.00 |
0.00 | 0.00 | 9.86 |
Polycrystalline dielectric constant
εpoly∞
6.73
|
Polycrystalline dielectric constant
εpoly
10.52
|
Refractive Index n2.60 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr(GaTe2)2 (mp-6987) | 0.2673 | 0.000 | 3 |
Ba(GaTe2)2 (mp-38117) | 0.2239 | 0.000 | 3 |
Ba(AlTe2)2 (mp-38394) | 0.2209 | 0.009 | 3 |
Sr(GaTe2)2 (mp-33880) | 0.2567 | 0.012 | 3 |
Sr(AlTe2)2 (mp-37091) | 0.2420 | 0.000 | 3 |
K2NbCuS4 (mp-9763) | 0.6419 | 0.000 | 4 |
Cs2LiVS4 (mp-510338) | 0.6380 | 0.000 | 4 |
Rb2TaCuS4 (mp-11923) | 0.6330 | 0.000 | 4 |
K2VCuS4 (mp-15147) | 0.6257 | 0.000 | 4 |
Rb2VCuS4 (mp-15219) | 0.6052 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Al Te |
Final Energy/Atom-4.0398 eV |
Corrected Energy-56.5575 eV
-56.5575 eV = -56.5575 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)