Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.170 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.434 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 136.1 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 191.9 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 166.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 319.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 317.7 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 325.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 136.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 299.6 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 319.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 130.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 215.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 299.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 277.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 185.1 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 266.3 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 336.3 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 136.1 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 216.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 246.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 299.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 130.4 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 195.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 199.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 92.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 266.3 |
Te2W (mp-22693) | <1 1 0> | <1 0 0> | 112.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 260.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 154.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 272.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 246.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 185.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 191.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 266.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 317.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 215.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 130.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 215.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 246.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 255.9 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 99.9 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 280.2 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 277.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 30.8 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 136.1 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 191.9 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 255.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 246.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 215.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 33.3 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 224.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
4.65 | 0.00 | 0.00 |
0.00 | 4.64 | 0.00 |
0.00 | 0.00 | 4.58 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.36 | 0.00 | 0.00 |
0.00 | 11.28 | 0.00 |
0.00 | 0.00 | 10.10 |
Polycrystalline dielectric constant
εpoly∞
4.62
|
Polycrystalline dielectric constant
εpoly
10.58
|
Refractive Index n2.15 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaLiTe (mp-8754) | 0.0915 | 0.000 | 3 |
KNaTe (mp-8755) | 0.0849 | 0.000 | 3 |
BaCaSn (mp-11265) | 0.1526 | 0.000 | 3 |
KNaS (mp-28383) | 0.1245 | 0.000 | 3 |
KNaSe (mp-28595) | 0.1170 | 0.000 | 3 |
Na2LiGaAs2 (mp-9722) | 0.4420 | 0.000 | 4 |
Na2LiAlP2 (mp-9719) | 0.5063 | 0.000 | 4 |
KNa4SnSb3 (mp-6758) | 0.4709 | 0.005 | 4 |
K2LiInAs2 (mp-505431) | 0.5089 | 0.000 | 4 |
K3Na2SnBi3 (mp-568329) | 0.4964 | 0.000 | 4 |
YbH2 (mp-864603) | 0.4079 | 0.000 | 2 |
CaH2 (mp-23713) | 0.3735 | 0.000 | 2 |
SrH2 (mp-23714) | 0.3751 | 0.000 | 2 |
Eu2Ge (mp-1095642) | 0.4463 | 0.000 | 2 |
BaH2 (mp-23715) | 0.4030 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Li_sv Se |
Final Energy/Atom-3.4093 eV |
Corrected Energy-42.7992 eV
Uncorrected energy = -40.9112 eV
Composition-based energy adjustment (-0.472 eV/atom x 4.0 atoms) = -1.8880 eV
Corrected energy = -42.7992 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)