Final Magnetic Moment0.120 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.196 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTl(CuSe)2 + Cu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 217.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 149.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 298.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 217.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 298.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 223.7 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 298.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 -1> | 298.3 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 289.6 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 289.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 289.6 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 298.3 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 298.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 298.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 289.6 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 290.1 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 298.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 289.6 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 223.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 289.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 223.7 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 217.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 144.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 289.6 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 -1> | 298.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 -1> | 223.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 144.8 |
GaP (mp-2490) | <1 0 0> | <1 0 -1> | 149.1 |
GaP (mp-2490) | <1 1 0> | <1 0 -1> | 298.3 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 -1> | 298.3 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 -1> | 223.7 |
C (mp-48) | <0 0 1> | <0 0 1> | 289.6 |
C (mp-48) | <1 0 1> | <0 0 1> | 217.2 |
C (mp-48) | <1 1 0> | <1 0 -1> | 298.3 |
C (mp-48) | <1 1 1> | <1 0 -1> | 298.3 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 289.6 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 -1> | 298.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 144.8 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 -1> | 149.1 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 -1> | 298.3 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 -1> | 298.3 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 -1> | 298.3 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 289.6 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 290.1 |
Si (mp-149) | <1 0 0> | <1 0 -1> | 149.1 |
Si (mp-149) | <1 1 0> | <1 0 -1> | 298.3 |
GaTe (mp-542812) | <1 0 0> | <1 0 -1> | 223.7 |
C (mp-48) | <1 0 0> | <1 0 1> | 248.6 |
CaF2 (mp-2741) | <1 0 0> | <1 0 -1> | 149.1 |
CaF2 (mp-2741) | <1 1 0> | <1 0 -1> | 298.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb3(Cu4S3)2 (mp-562230) | 0.6160 | 0.000 | 3 |
Rb3(Cu4Se3)2 (mp-616220) | 0.4361 | 0.000 | 3 |
Tb2Mg3Ni2 (mp-570272) | 0.7077 | 0.000 | 3 |
K3(Cu4Se3)2 (mp-4647) | 0.3217 | 0.012 | 3 |
TlCu3Se2 (mp-8800) | 0.6958 | 0.027 | 3 |
MgSi2 (mp-1073465) | 0.6304 | 0.256 | 2 |
Mg5Si6 (mp-31404) | 0.7112 | 0.238 | 2 |
K4Pb9 (mp-680443) | 0.7060 | 0.007 | 2 |
Rb4Pb9 (mp-680463) | 0.6591 | 0.000 | 2 |
Mg4Si3 (mp-1074333) | 0.6878 | 0.121 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Cu_pv Se |
Final Energy/Atom-3.7880 eV |
Corrected Energy-109.8533 eV
-109.8533 eV = -109.8533 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)