Final Magnetic Moment2.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.989 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 139.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 274.4 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 113.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 262.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 274.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 262.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 253.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 274.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 274.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 -1> | 226.2 |
Al (mp-134) | <1 1 0> | <1 1 0> | 253.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 113.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 139.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 91.5 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 262.8 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 226.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 164.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 274.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 -1> | 113.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 139.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 -1> | 226.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 -1> | 226.2 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 -1> | 113.1 |
KP(HO2)2 (mp-23959) | <1 0 1> | <0 0 1> | 139.8 |
KP(HO2)2 (mp-23959) | <1 1 0> | <0 0 1> | 139.8 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 274.4 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 -1> | 143.0 |
SiC (mp-11714) | <1 1 0> | <1 0 -1> | 113.1 |
SiC (mp-11714) | <1 0 1> | <1 0 -1> | 226.2 |
C (mp-48) | <0 0 1> | <1 0 -1> | 226.2 |
C (mp-48) | <1 0 0> | <0 1 0> | 175.2 |
Au (mp-81) | <1 0 0> | <1 0 0> | 274.4 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 262.8 |
ZrO2 (mp-2858) | <1 0 -1> | <1 1 0> | 253.3 |
C (mp-48) | <1 1 1> | <1 0 0> | 274.4 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 -1> | 113.1 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 -1> | 113.1 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 -1> | 113.1 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 274.4 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 139.8 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 262.8 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 262.8 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 0> | 274.4 |
GaTe (mp-542812) | <1 0 0> | <1 0 0> | 91.5 |
ZnTe (mp-2176) | <1 0 0> | <0 1 0> | 262.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaYF5 (mp-752675) | 0.6406 | 0.000 | 3 |
BaTbF6 (mp-8573) | 0.7453 | 0.041 | 3 |
CeSmI4 (mp-570470) | 0.7255 | 0.080 | 3 |
CeNdI4 (mp-570728) | 0.7182 | 0.081 | 3 |
Cu2PPd2 (mp-1001022) | 0.6952 | 0.004 | 3 |
HfF4 (mp-31033) | 0.1229 | 0.000 | 2 |
ThF4 (mp-31034) | 0.1349 | 0.000 | 2 |
CeF4 (mp-542001) | 0.1280 | 0.000 | 2 |
NpF4 (mp-504787) | 0.1186 | 0.000 | 2 |
NpF4 (mp-864802) | 0.3797 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U F |
Final Energy/Atom-7.3834 eV |
Corrected Energy-221.5016 eV
-221.5016 eV = -221.5016 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)