Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.290 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.705 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 249.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 166.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 161.4 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 249.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 168.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 83.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 118.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 166.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 161.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 182.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 166.5 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 249.8 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 118.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 166.5 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 166.5 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 182.0 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 84.2 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 249.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 249.8 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 118.4 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 161.4 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 161.4 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 249.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 249.8 |
TiO2 (mp-390) | <1 1 0> | <0 1 0> | 252.5 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 83.3 |
MgF2 (mp-1249) | <1 1 1> | <1 1 0> | 118.4 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 118.4 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 168.4 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 166.5 |
LaF3 (mp-905) | <0 0 1> | <0 1 1> | 182.0 |
LaF3 (mp-905) | <1 1 0> | <1 0 1> | 182.5 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 249.8 |
Al2O3 (mp-1143) | <1 0 0> | <0 1 0> | 252.5 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 249.8 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 161.4 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 249.8 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 249.8 |
WS2 (mp-224) | <1 0 0> | <0 1 1> | 182.0 |
C (mp-48) | <0 0 1> | <1 1 0> | 236.8 |
C (mp-48) | <1 0 0> | <1 0 0> | 249.8 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 161.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
7.05 | -0.00 | -0.02 |
-0.00 | 6.98 | -0.00 |
-0.02 | -0.00 | 10.45 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.78 | -0.00 | 0.03 |
-0.00 | 11.45 | -0.00 |
0.03 | -0.00 | 20.67 |
Polycrystalline dielectric constant
εpoly∞
8.16
|
Polycrystalline dielectric constant
εpoly
14.63
|
Refractive Index n2.86 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbMg6Cu (mp-1022140) | 0.6602 | 0.271 | 3 |
BaMg6Ni (mp-1022026) | 0.6524 | 0.206 | 3 |
Tl5Se2Cl (mp-28920) | 0.5365 | 0.000 | 3 |
RbMg6Si (mp-1098280) | 0.6707 | 0.306 | 3 |
CsRbMg6 (mp-1098082) | 0.6459 | 0.280 | 3 |
Sn3Ru2 (mp-680677) | 0.5564 | 0.002 | 2 |
Si3Ru2 (mp-20191) | 0.5773 | 0.022 | 2 |
Ge3Ru2 (mp-706531) | 0.5184 | 0.003 | 2 |
Ge3Os2 (mp-510032) | 0.5371 | 0.012 | 2 |
Si3Os2 (mp-16609) | 0.5843 | 0.030 | 2 |
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Os_pv Br |
Final Energy/Atom-6.1389 eV |
Corrected Energy-114.7718 eV
Uncorrected energy = -110.4998 eV
Composition-based energy adjustment (-0.534 eV/atom x 8.0 atoms) = -4.2720 eV
Corrected energy = -114.7718 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)