Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.797 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.703 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 289.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 289.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 146.8 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 220.6 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 175.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 275.7 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 275.7 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 275.7 |
BN (mp-984) | <1 0 0> | <1 0 0> | 96.4 |
Al (mp-134) | <1 0 0> | <0 1 0> | 146.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 96.4 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 275.7 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 220.6 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 275.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 275.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 192.8 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 173.2 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 110.3 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 96.4 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 289.1 |
Ni (mp-23) | <1 0 0> | <1 1 -1> | 183.6 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 173.2 |
InSb (mp-20012) | <1 0 0> | <1 0 -1> | 220.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 175.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 192.8 |
Si (mp-149) | <1 1 0> | <1 0 0> | 289.1 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 -1> | 110.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 192.8 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 289.1 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 -1> | 110.3 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 91.9 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 289.1 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 289.1 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 275.7 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 183.8 |
ZnO (mp-2133) | <1 0 0> | <0 1 1> | 173.2 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 275.7 |
Cu (mp-30) | <1 0 0> | <1 0 -1> | 220.6 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 -1> | 110.3 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 96.4 |
LiAlO2 (mp-3427) | <1 1 1> | <1 0 -1> | 110.3 |
Fe2O3 (mp-24972) | <1 0 1> | <1 0 -1> | 220.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb3BiBr6 (mp-27147) | 0.4017 | 0.000 | 3 |
K3MoCl6 (mp-27643) | 0.2653 | 0.133 | 3 |
Rb3TlCl6 (mp-29384) | 0.1968 | 0.000 | 3 |
Cs3NdCl6 (mp-582081) | 0.4411 | 0.000 | 3 |
K3IrCl6 (mp-541141) | 0.1195 | 0.000 | 3 |
CsK2BiCl6 (mp-571371) | 0.7042 | 0.000 | 4 |
NaSrCrF6 (mp-561262) | 0.7348 | 0.113 | 4 |
Na3Pr14(RuO6)6 (mp-554060) | 0.6464 | 0.064 | 4 |
K4SnSb2F14 (mp-558309) | 0.7144 | 0.000 | 4 |
Na3Nd14(RuO6)6 (mp-555804) | 0.6616 | 0.000 | 4 |
Tl2Br3 (mp-680345) | 0.6302 | 0.013 | 2 |
In2Cl3 (mp-667324) | 0.7272 | 0.003 | 2 |
Tl2Cl3 (mp-680294) | 0.7245 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Rh_pv Cl |
Final Energy/Atom-3.6159 eV |
Corrected Energy-159.3735 eV
Uncorrected energy = -144.6375 eV
Composition-based energy adjustment (-0.614 eV/atom x 24.0 atoms) = -14.7360 eV
Corrected energy = -159.3735 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)