Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.274 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHgCl + P + Hg |
Band Gap1.184 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 0> | 186.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 279.2 |
BaF2 (mp-1029) | <1 1 1> | <1 0 -1> | 279.7 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 223.7 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 247.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 209.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 279.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 189.6 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 279.2 |
KCl (mp-23193) | <1 1 1> | <1 0 -1> | 279.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 209.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 213.5 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 279.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 209.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 209.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 215.7 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 279.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 185.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 185.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 308.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 279.2 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 284.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 279.2 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 279.2 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 279.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 69.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 209.4 |
BN (mp-984) | <1 0 1> | <1 1 0> | 279.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 247.1 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 93.2 |
Al (mp-134) | <1 0 0> | <1 1 1> | 246.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 185.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 -1> | 111.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 287.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 215.7 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 279.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 279.7 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 287.7 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 189.6 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 -1> | 93.2 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 279.2 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 308.9 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 279.7 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 287.7 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 308.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 215.7 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 1> | 213.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 308.9 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 247.1 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 247.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K2In2As3 (mp-21741) | 0.6313 | 0.000 | 3 |
Hg2As3Br (mp-28899) | 0.2723 | 0.000 | 3 |
K2In2Sb3 (mp-579637) | 0.6272 | 0.000 | 3 |
Na2MnO2 (mp-565246) | 0.5870 | 0.006 | 3 |
Na2Ga2As3 (mp-15431) | 0.6235 | 0.000 | 3 |
K2Li3MnO4 (mp-773442) | 0.5835 | 0.174 | 4 |
Ag2Bi2S3Cl2 (mp-559071) | 0.6480 | 0.000 | 4 |
K2In3AgSe6 (mp-680403) | 0.6394 | 0.009 | 4 |
K3Na2InO4 (mp-553975) | 0.5377 | 0.000 | 4 |
LiCaAlN2 (mp-1020031) | 0.5893 | 0.000 | 4 |
In4Te3 (mp-617281) | 0.7306 | 0.000 | 2 |
MgSi2 (mp-1073530) | 0.7133 | 0.234 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hg P Cl |
Final Energy/Atom-3.2912 eV |
Corrected Energy-40.7224 eV
Uncorrected energy = -39.4944 eV
Composition-based energy adjustment (-0.614 eV/atom x 2.0 atoms) = -1.2280 eV
Corrected energy = -40.7224 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)