Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.262 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.008 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb2Te5 + Te |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 170.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 281.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 187.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 272.0 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 152.9 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 103.1 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 103.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 272.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 93.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 281.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 272.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 90.7 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 281.1 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 281.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 93.7 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 272.0 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 152.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 181.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 0 0> | 187.4 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 281.1 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 90.7 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 272.0 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 281.1 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 90.7 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 187.4 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 187.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 272.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 272.0 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 272.0 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 272.0 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 281.1 |
C (mp-48) | <1 0 0> | <1 1 0> | 171.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 272.0 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 0 0> | 187.4 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 281.1 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 1> | 152.9 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 272.0 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 272.0 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 272.0 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 90.7 |
CdWO4 (mp-19387) | <1 1 1> | <1 0 -1> | 103.1 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 181.3 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 281.1 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 281.1 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 272.0 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 272.0 |
LiAlO2 (mp-3427) | <1 1 0> | <1 0 0> | 93.7 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 281.1 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 -1> | 206.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K(SbSe2)2 (mp-9797) | 0.7062 | 0.000 | 3 |
RbBiF3 (mp-677028) | 0.7391 | 0.133 | 3 |
TlSb3S5 (mp-27515) | 0.7385 | 0.004 | 3 |
Nd2Ge2Ir (mp-22768) | 0.7296 | 0.366 | 3 |
K5Sb4 (mp-685149) | 0.7464 | 0.051 | 2 |
MgSi (mp-1073799) | 0.7244 | 0.125 | 2 |
MgSi (mp-1073750) | 0.7176 | 0.135 | 2 |
Mg4Si3 (mp-1074264) | 0.6975 | 0.152 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Te |
Final Energy/Atom-3.0962 eV |
Corrected Energy-43.3473 eV
-43.3473 eV = -43.3473 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)