Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.703 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.242 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/m [10] |
Hall-P 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 83.7 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 135.4 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 167.4 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 286.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 307.5 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 316.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 316.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 87.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 307.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 256.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 167.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 238.6 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 290.8 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 290.8 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 180.6 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 180.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 219.6 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 174.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 219.6 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 330.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 300.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 43.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 219.6 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 225.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 270.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 330.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 286.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 190.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 167.4 |
GaSe (mp-1943) | <1 1 1> | <1 0 0> | 225.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 146.7 |
BN (mp-984) | <1 0 1> | <0 1 0> | 183.3 |
BN (mp-984) | <1 1 0> | <0 1 0> | 293.4 |
BN (mp-984) | <1 1 1> | <1 0 1> | 300.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 293.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 131.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 225.7 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 238.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 330.0 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 0> | 256.7 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 232.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 175.7 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 240.7 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 316.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 293.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 183.3 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 131.8 |
MoS2 (mp-1434) | <1 1 0> | <1 0 1> | 225.6 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 290.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 220.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn(CoO2)2 (mp-767807) | 0.4472 | 0.015 | 3 |
Mn2CoO4 (mp-767836) | 0.4457 | 0.038 | 3 |
MgMn2O4 (mvc-10190) | 0.4427 | 0.035 | 3 |
Mn2ZnO4 (mvc-10371) | 0.4406 | 0.048 | 3 |
LiMn2O4 (mp-1097867) | 0.4407 | 0.000 | 3 |
Li4Ni8O9F7 (mp-764792) | 0.4009 | 0.067 | 4 |
Li4Fe5Sb3O16 (mp-770140) | 0.4090 | 0.040 | 4 |
LiMn2O3F (mp-766865) | 0.3592 | 0.083 | 4 |
Li3Mn3O3F5 (mp-766975) | 0.3717 | 0.064 | 4 |
Li2Mn4O5F3 (mp-763883) | 0.4039 | 0.091 | 4 |
NiP4 (mp-770274) | 0.5297 | 0.087 | 2 |
FeP4 (mp-27164) | 0.4996 | 0.001 | 2 |
P4Ru (mp-27173) | 0.4857 | 0.000 | 2 |
NiP4 (mp-769108) | 0.5225 | 0.078 | 2 |
FeP4 (mp-570553) | 0.5503 | 0.000 | 2 |
Li4Mn3V2Sb3O16 (mp-775695) | 0.4047 | 0.061 | 5 |
Li4Mn3Cr2Sb3O16 (mp-764395) | 0.3890 | 0.073 | 5 |
Li4Mn3Fe2Sb3O16 (mp-775443) | 0.4128 | 0.062 | 5 |
Li4Fe2Ni3Sb3O16 (mp-764048) | 0.4215 | 0.047 | 5 |
Li4Fe2Cu3Sb3O16 (mp-767936) | 0.4134 | 0.082 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv Pt S |
Final Energy/Atom-5.0078 eV |
Corrected Energy-75.4174 eV
-75.4174 eV = -70.1097 eV (uncorrected energy) - 5.3077 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)