material

CuBIr

ID:

mp-28896

DOI:

10.17188/1202972


Tags: Copper(I) iridium(II) boride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.188 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.36 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fdd2 [43]
Hall
F 2 2d
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 75029 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <1 0 1> <1 0 1> 0.012 209.1
ZnO (mp-2133) <0 0 1> <0 1 1> 0.019 261.2
BN (mp-984) <0 0 1> <1 0 0> 0.026 87.5
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.028 87.5
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.057 286.5
TiO2 (mp-2657) <0 0 1> <0 1 1> 0.062 87.1
AlN (mp-661) <1 1 0> <1 1 0> 0.070 109.3
GaSe (mp-1943) <0 0 1> <0 1 0> 0.082 327.8
InAs (mp-20305) <1 1 1> <1 0 0> 0.086 262.4
Ni (mp-23) <1 0 0> <0 1 0> 0.090 196.7
SiC (mp-8062) <1 0 0> <0 1 1> 0.091 174.2
Au (mp-81) <1 0 0> <0 1 0> 0.097 262.3
ZnTe (mp-2176) <1 1 1> <1 0 0> 0.101 262.4
TePb (mp-19717) <1 0 0> <0 1 1> 0.104 87.1
SiO2 (mp-6930) <1 1 1> <1 0 1> 0.115 104.6
CaCO3 (mp-3953) <0 0 1> <1 0 0> 0.116 87.5
CdWO4 (mp-19387) <1 1 0> <0 1 0> 0.122 327.8
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.127 109.3
SiC (mp-11714) <1 0 1> <0 0 1> 0.129 229.2
CdTe (mp-406) <1 0 0> <0 1 1> 0.135 87.1
C (mp-66) <1 1 1> <1 0 0> 0.136 87.5
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.137 286.5
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.151 109.3
Ag (mp-124) <1 0 0> <0 1 0> 0.151 262.3
InSb (mp-20012) <1 0 0> <0 1 1> 0.159 87.1
SiC (mp-11714) <1 0 0> <1 1 0> 0.160 218.6
Mg (mp-153) <1 0 0> <0 0 1> 0.172 286.5
Ni (mp-23) <1 1 1> <0 0 1> 0.186 171.9
MgF2 (mp-1249) <0 0 1> <0 1 1> 0.192 87.1
TbScO3 (mp-31119) <0 1 1> <1 1 0> 0.193 109.3
ZnO (mp-2133) <1 0 0> <0 0 1> 0.211 171.9
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.229 286.5
GdScO3 (mp-5690) <1 1 1> <1 1 0> 0.241 218.6
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.279 57.3
Ni (mp-23) <1 1 0> <1 0 1> 0.282 104.6
Cu (mp-30) <1 0 0> <1 0 0> 0.292 262.4
Ga2O3 (mp-886) <0 1 0> <1 0 1> 0.296 209.1
CdSe (mp-2691) <1 1 1> <1 0 0> 0.296 262.4
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.300 109.3
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.305 286.5
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.311 286.5
Al (mp-134) <1 1 0> <1 0 1> 0.313 209.1
GaN (mp-804) <0 0 1> <0 0 1> 0.317 286.5
LiGaO2 (mp-5854) <0 1 0> <0 1 0> 0.323 65.6
Ag (mp-124) <1 1 0> <1 1 0> 0.331 218.6
LiGaO2 (mp-5854) <1 1 0> <0 1 0> 0.346 196.7
Te2Mo (mp-602) <1 0 1> <0 1 0> 0.352 327.8
GaSb (mp-1156) <1 1 1> <1 0 0> 0.356 262.4
LaF3 (mp-905) <1 0 0> <0 1 0> 0.360 327.8
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.363 209.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
270 110 179 0 0 0
110 280 148 0 0 0
179 148 326 0 0 0
0 0 0 41 0 0
0 0 0 0 109 0
0 0 0 0 0 62
Compliance Tensor Sij (10-12Pa-1)
6 -0.8 -2.9 0 0 0
-0.8 4.8 -1.7 0 0 0
-2.9 -1.7 5.5 0 0 0
0 0 0 24.1 0 0
0 0 0 0 9.2 0
0 0 0 0 0 16.1
Shear Modulus GV
72 GPa
Bulk Modulus KV
194 GPa
Shear Modulus GR
64 GPa
Bulk Modulus KR
188 GPa
Shear Modulus GVRH
68 GPa
Bulk Modulus KVRH
191 GPa
Elastic Anisotropy
0.66
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CeSI (mp-680698) 0.5381 0.020 3
NdSBr (mp-27180) 0.4680 0.000 3
BIrPd (mp-28897) 0.2188 0.000 3
Na2ZnSe2 (mp-1024052) 0.5086 0.000 3
ScOF (mp-4661) 0.5495 0.000 3
CaBiClO2 (mp-553025) 0.7074 0.000 4
KNaZnO2 (mp-557183) 0.7065 0.000 4
LiCaGaN2 (mp-570948) 0.6445 0.000 4
LiCaAlN2 (mp-1020031) 0.6385 0.000 4
ZrO2 (mp-2858) 0.6882 0.000 2
HfO2 (mp-352) 0.6968 0.000 2
ZrO2 (mp-776404) 0.6916 0.009 2
NdO2 (mp-755820) 0.6739 0.169 2
CeSe2 (mp-1080853) 0.6804 0.029 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv B Ir
Final Energy/Atom
-6.7270 eV
Corrected Energy
-80.7237 eV
-80.7237 eV = -80.7237 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 75029
Submitted by
User remarks:
  • Copper(I) iridium(II) boride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)