material

K3BiSe3

ID:

mp-28980

DOI:

10.17188/1203036


Tags: Tripotassium catena-triselenobismuthate(III)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.952 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.78 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.068 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P213 [198]
Hall
P 2ac 2ab 3
Point Group
23
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.000 198.2
GaAs (mp-2534) <1 1 1> <1 1 1> 0.000 171.6
GaAs (mp-2534) <1 1 0> <1 1 0> 0.000 140.1
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.000 171.6
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.000 140.1
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.003 198.2
Ge (mp-32) <1 1 1> <1 1 1> 0.005 171.6
Ge (mp-32) <1 1 0> <1 1 0> 0.005 140.1
Ni (mp-23) <1 1 0> <1 1 0> 0.007 140.1
Ni (mp-23) <1 0 0> <1 0 0> 0.007 99.1
LiF (mp-1138) <1 1 0> <1 1 0> 0.015 140.1
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.017 140.1
Al (mp-134) <1 1 0> <1 1 0> 0.024 140.1
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.049 198.2
NaCl (mp-22862) <1 1 1> <1 1 1> 0.058 171.6
NaCl (mp-22862) <1 1 0> <1 1 0> 0.059 140.1
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.065 297.3
PbSe (mp-2201) <1 0 0> <1 0 0> 0.078 198.2
GaSb (mp-1156) <1 0 0> <1 0 0> 0.097 198.2
AlN (mp-661) <0 0 1> <1 0 0> 0.097 297.3
CdSe (mp-2691) <1 0 0> <1 0 0> 0.113 198.2
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.131 297.3
Ag (mp-124) <1 1 1> <1 0 0> 0.146 297.3
TiO2 (mp-390) <1 0 0> <1 0 0> 0.161 297.3
KCl (mp-23193) <1 0 0> <1 0 0> 0.168 198.2
Au (mp-81) <1 1 1> <1 0 0> 0.168 297.3
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.183 297.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
23 7 7 0 0 0
7 23 7 0 0 0
7 7 23 0 0 0
0 0 0 6 0 0
0 0 0 0 6 0
0 0 0 0 0 6
Compliance Tensor Sij (10-12Pa-1)
50.9 -12 -12 0 0 0
-12 50.9 -12 0 0 0
-12 -12 50.9 0 0 0
0 0 0 167.1 0 0
0 0 0 0 167.1 0
0 0 0 0 0 167.1
Shear Modulus GV
7 GPa
Bulk Modulus KV
12 GPa
Shear Modulus GR
7 GPa
Bulk Modulus KR
12 GPa
Shear Modulus GVRH
7 GPa
Bulk Modulus KVRH
12 GPa
Elastic Anisotropy
0.10
Poisson's Ratio
0.27

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.07601 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.07601 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.07601
Piezoelectric Modulus ‖eijmax
0.07601 C/m2
Crystallographic Direction vmax
1.00000
0.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.58 0.00 0.00
0.00 4.58 0.00
0.00 0.00 4.58
Dielectric Tensor εij (total)
9.48 0.00 0.00
0.00 9.48 0.00
0.00 0.00 9.48
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.58
Polycrystalline dielectric constant εpoly
(total)
9.48
Refractive Index n
2.14
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
K3SbTe3 (mp-5626) 0.1987 0.000 3
K3SbSe3 (mp-17538) 0.2679 0.000 3
Rb3BiSe3 (mp-29168) 0.1854 0.000 3
K3BiTe3 (mp-29379) 0.1737 0.000 3
Na3AsS3 (mp-5830) 0.3108 0.000 3
KEuAsS3 (mp-646548) 0.7189 0.001 4
RbEuAsS3 (mp-646129) 0.7470 0.000 4
K2RbBiSe3 (mp-621964) 0.1179 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: K_sv Bi Se
Final Energy/Atom
-3.4816 eV
Corrected Energy
-103.1490 eV
Uncorrected energy = -97.4850 eV Composition-based energy adjustment (-0.472 eV/atom x 12.0 atoms) = -5.6640 eV Corrected energy = -103.1490 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 78841
Submitted by
User remarks:
  • Tripotassium catena-triselenobismuthate(III)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)