Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.520 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.757 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 1> | 232.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 150.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 100.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 250.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 310.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 237.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 200.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 237.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 50.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 118.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 300.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 250.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 237.2 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 296.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 50.1 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 118.6 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 237.2 |
BN (mp-984) | <1 1 1> | <0 1 0> | 237.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 310.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 50.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 118.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 310.5 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 186.9 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 296.5 |
C (mp-66) | <1 1 0> | <0 1 0> | 177.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 1> | 310.5 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 180.1 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 180.1 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 150.3 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 296.5 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 150.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 237.2 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 310.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 150.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 100.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 186.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 250.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 177.9 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 186.9 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 118.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 118.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 300.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 310.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 310.5 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 189.6 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 100.2 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 150.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 250.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 300.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba(LuS2)2 (mp-984052) | 0.0972 | 0.000 | 3 |
Sr(YS2)2 (mp-29035) | 0.1243 | 0.000 | 3 |
Sr(ScS2)2 (mp-17678) | 0.1134 | 0.000 | 3 |
CaCr2O4 (mvc-11432) | 0.1314 | 0.005 | 3 |
Sr(DyS2)2 (mp-980666) | 0.1262 | 0.000 | 3 |
Ca5Sc2(CoO6)2 (mvc-13126) | 0.6799 | 0.027 | 4 |
Na3Mn4(TeO6)2 (mp-565229) | 0.6085 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Y_sv S |
Final Energy/Atom-6.6258 eV |
Corrected Energy-196.1382 eV
-196.1382 eV = -185.5228 eV (uncorrected energy) - 10.6154 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)