Final Magnetic Moment3.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.999 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVCl2 + LiCl |
Band Gap1.589 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 213.5 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 184.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 106.7 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 184.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 213.5 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 184.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 213.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 213.5 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 106.7 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 184.9 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 184.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 150.9 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 184.9 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 150.9 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 184.9 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 213.5 |
WS2 (mp-224) | <0 0 1> | <1 1 1> | 184.9 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 106.7 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 150.9 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 184.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.06 | 0.00 | 0.00 |
0.00 | 3.06 | -0.00 |
0.00 | -0.00 | 3.06 |
Dielectric Tensor εij (total) |
||
---|---|---|
11.38 | 0.00 | 0.00 |
0.00 | 11.38 | -0.00 |
0.00 | -0.00 | 11.38 |
Polycrystalline dielectric constant
εpoly∞
3.06
|
Polycrystalline dielectric constant
εpoly
11.38
|
Refractive Index n1.75 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li6CuF8 (mp-753139) | 0.0429 | 0.036 | 3 |
Li6FeCl8 (mp-28828) | 0.0046 | 0.092 | 3 |
Li6MgBr8 (mp-29008) | 0.0392 | 0.020 | 3 |
Li6CoCl8 (mp-505391) | 0.0474 | 0.031 | 3 |
Li6VF8 (mp-765804) | 0.0937 | 0.056 | 3 |
Li3VCr3O8 (mp-771672) | 0.2819 | 0.038 | 4 |
Li3Cr2(FeO4)2 (mp-780017) | 0.2673 | 1.106 | 4 |
Li2Ti4VO8 (mp-768018) | 0.2283 | 0.105 | 4 |
Li3VFe3O8 (mp-773273) | 0.2589 | 0.072 | 4 |
Li3Cr3FeO8 (mp-853144) | 0.2773 | 0.582 | 4 |
Fe7O8 (mp-705548) | 0.0785 | 0.099 | 2 |
Zr10C9 (mp-684623) | 0.2220 | 0.000 | 2 |
V8C7 (mp-542730) | 0.2733 | 0.007 | 2 |
Fe7O8 (mp-32939) | 0.1265 | 0.099 | 2 |
Ni9O10 (mp-656884) | 0.2535 | 0.047 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.7085 | 0.882 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv V_pv Cl |
Final Energy/Atom-4.0371 eV |
Corrected Energy-65.4689 eV
Uncorrected energy = -60.5569 eV
Composition-based energy adjustment (-0.614 eV/atom x 8.0 atoms) = -4.9120 eV
Corrected energy = -65.4689 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)