Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.349 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.10 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToKBi + K3Bi + K2SnBi |
Band Gap0.014 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 275.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 170.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 275.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 174.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 174.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 275.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 275.7 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 170.4 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 170.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 275.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 275.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 275.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 275.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 91.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 174.7 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 174.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 275.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 275.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 275.7 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 193.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 275.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 170.4 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 275.7 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 275.7 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 0> | 170.4 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 170.4 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 91.9 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 275.7 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 275.7 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 275.7 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 91.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 183.8 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 275.7 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 275.7 |
LiAlO2 (mp-3427) | <1 0 1> | <0 1 0> | 170.4 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 275.7 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 170.4 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 275.7 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 91.9 |
Fe2O3 (mp-24972) | <1 0 0> | <0 0 1> | 275.7 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 275.7 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 275.7 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 275.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 275.7 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 275.7 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 170.4 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 -1> | 148.8 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 183.8 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 275.7 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 275.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na5GeP3 (mp-4172) | 0.4292 | 0.000 | 3 |
K5SnSb3 (mp-5367) | 0.2594 | 0.002 | 3 |
Na5GeAs3 (mp-16861) | 0.4581 | 0.000 | 3 |
K5SnAs3 (mp-16989) | 0.3396 | 0.000 | 3 |
Na5SiAs3 (mp-18139) | 0.4373 | 0.000 | 3 |
KNa4SnSb3 (mp-6758) | 0.6227 | 0.005 | 4 |
Cs3Na2SnP3 (mp-17707) | 0.6264 | 0.000 | 4 |
Rb5Ta(TlAs2)2 (mp-570566) | 0.5675 | 0.000 | 4 |
K3Na2SnP3 (mp-16847) | 0.6165 | 0.000 | 4 |
K6NbTlAs4 (mp-567820) | 0.6007 | 0.000 | 4 |
Mg2Si3 (mp-1072992) | 0.5493 | 0.270 | 2 |
Mg4Si3 (mp-1074264) | 0.6356 | 0.152 | 2 |
Mg3Si4 (mp-1075009) | 0.6487 | 0.191 | 2 |
Mg5Si6 (mp-1075466) | 0.6316 | 0.195 | 2 |
Mg5Si9 (mp-1075612) | 0.6258 | 0.234 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Sn_d Bi |
Final Energy/Atom-2.7085 eV |
Corrected Energy-97.5064 eV
-97.5064 eV = -97.5064 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)