Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.765 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.845 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 99.1 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 198.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 198.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 297.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 297.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 198.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 198.2 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 198.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 198.2 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 198.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 173.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 173.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 99.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 198.2 |
Al (mp-134) | <1 1 1> | <1 0 0> | 198.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 99.1 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 297.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 199.9 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 173.6 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 297.3 |
C (mp-66) | <1 1 1> | <1 0 0> | 198.2 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 173.6 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 0 0> | 198.2 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 0> | 297.3 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 297.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 297.3 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 297.3 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 297.3 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 173.6 |
PbSe (mp-2201) | <1 1 1> | <1 0 0> | 198.2 |
Si (mp-149) | <1 0 0> | <1 0 0> | 297.3 |
Si (mp-149) | <1 1 1> | <1 0 0> | 99.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 173.6 |
CdSe (mp-2691) | <1 1 1> | <1 0 0> | 198.2 |
WSe2 (mp-1821) | <1 0 0> | <1 0 1> | 199.9 |
C (mp-48) | <1 1 0> | <1 0 1> | 199.9 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 198.2 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 198.2 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 198.2 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 173.6 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 297.3 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 173.6 |
ZnO (mp-2133) | <0 0 1> | <1 0 0> | 198.2 |
GaSb (mp-1156) | <1 1 1> | <1 0 0> | 198.2 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 297.3 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 0> | 140.2 |
ZnTe (mp-2176) | <1 1 1> | <1 0 0> | 198.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbCl4F (mp-23412) | 0.3169 | 0.000 | 3 |
Sb2I2F11 (mp-27236) | 0.4419 | 0.017 | 3 |
TaCl4F (mp-27854) | 0.3465 | 0.000 | 3 |
ReO2F3 (mp-555704) | 0.4093 | 0.000 | 3 |
SbCl3F2 (mp-560748) | 0.1443 | 0.004 | 3 |
Cs2U(Br2O)2 (mp-572551) | 0.6044 | 0.000 | 4 |
Rb2Mn(Cl2O)2 (mp-1078743) | 0.5029 | 0.348 | 4 |
Cs2Mn(Cl2O)2 (mp-1080610) | 0.4599 | 0.342 | 4 |
SbMoOF9 (mp-567264) | 0.5813 | 0.000 | 4 |
TaF5 (mp-561197) | 0.4911 | 0.000 | 2 |
MoF5 (mp-555649) | 0.5027 | 0.078 | 2 |
VF5 (mp-765218) | 0.5429 | 0.013 | 2 |
NbF5 (mp-18687) | 0.4516 | 0.000 | 2 |
MoF5 (mp-608126) | 0.4986 | 0.078 | 2 |
K3VC5N5O (mp-705009) | 0.6140 | 0.274 | 5 |
HgSb4C2(OF11)2 (mp-556903) | 0.5983 | 0.080 | 5 |
K2IrCBr5O (mp-648833) | 0.6320 | 0.206 | 5 |
K2RuNCl5O (mp-541361) | 0.6199 | 0.000 | 5 |
K2RuNCl5O (mp-560966) | 0.6343 | 0.000 | 5 |
K3WC4N4OF (mp-651173) | 0.7451 | 0.255 | 6 |
Sb4IrC5ClO5F22 (mp-555612) | 0.7081 | 0.108 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb Cl F |
Final Energy/Atom-3.5538 eV |
Corrected Energy-96.3561 eV
Uncorrected energy = -85.2921 eV
Composition-based energy adjustment (-0.462 eV/atom x 8.0 atoms) = -3.6960 eV
Composition-based energy adjustment (-0.614 eV/atom x 12.0 atoms) = -7.3680 eV
Corrected energy = -96.3561 eV
|