Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.585 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCS14 + SCl + C |
Band Gap2.882 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 0> | <0 0 1> | 216.4 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 248.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 182.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 -1> | 182.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 165.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 248.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 -1> | 196.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 216.4 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 288.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 153.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 288.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 288.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 248.9 |
Al (mp-134) | <1 1 0> | <1 1 -1> | 182.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 216.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 288.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 288.5 |
C (mp-66) | <1 1 0> | <0 1 -1> | 196.8 |
Mg (mp-153) | <1 0 0> | <1 1 -1> | 182.5 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 248.9 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 216.4 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 248.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 248.9 |
Ga2O3 (mp-886) | <1 1 -1> | <1 -1 0> | 167.8 |
C (mp-48) | <0 0 1> | <0 0 1> | 216.4 |
NaCl (mp-22862) | <1 1 0> | <1 1 -1> | 182.5 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 248.9 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 288.5 |
YAlO3 (mp-3792) | <1 0 1> | <0 1 0> | 248.9 |
SiC (mp-8062) | <1 1 0> | <0 1 -1> | 295.2 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 248.9 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 -1> | 295.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 288.5 |
ZnO (mp-2133) | <1 0 1> | <0 1 -1> | 98.4 |
LiAlO2 (mp-3427) | <0 0 1> | <0 1 -1> | 295.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
H2CO (mp-995226) | 0.5037 | 0.345 | 3 |
H4C2O (mp-995220) | 0.5342 | 0.239 | 3 |
H2CO (mp-23683) | 0.4641 | 0.322 | 3 |
H2CO (mp-1096984) | 0.4103 | 0.337 | 3 |
C2(OF2)3 (mp-29479) | 0.3203 | 0.232 | 3 |
H2CSO4 (mp-995221) | 0.4802 | 0.305 | 4 |
FeS3N2Cl5 (mp-554079) | 0.6809 | 0.052 | 4 |
GaSe3N2Cl5 (mp-569902) | 0.6287 | 0.155 | 4 |
S4N2O3F (mp-555707) | 0.5352 | 0.105 | 4 |
FeS3(NCl2)2 (mp-556297) | 0.5135 | 0.062 | 4 |
CrO3 (mp-776563) | 0.7003 | 0.101 | 2 |
Ga3Cl7 (mp-616204) | 0.7221 | 0.010 | 2 |
P2S5 (mp-541788) | 0.3831 | 0.000 | 2 |
FeCl3 (mp-676241) | 0.5771 | 0.024 | 2 |
P2S7 (mp-1006118) | 0.6470 | 0.003 | 2 |
RbCdH2I3O (mp-634062) | 0.6987 | 0.003 | 5 |
FeTeS2N2Cl5 (mp-638705) | 0.6020 | 0.216 | 5 |
AlSeS2N2Cl5 (mp-556831) | 0.6659 | 0.075 | 5 |
H8CN2(ClO5)2 (mp-560730) | 0.6911 | 0.540 | 5 |
CS4N2(OF)3 (mp-555309) | 0.6530 | 0.203 | 5 |
CSe2S2N2(OF)3 (mp-555329) | 0.6594 | 0.222 | 6 |
PS2N3Cl2(OF)2 (mp-558888) | 0.7475 | 0.278 | 6 |
MnGe4H24C8(S5N)2 (mp-698410) | 0.6940 | 0.057 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: C S Cl |
Final Energy/Atom-3.9375 eV |
Corrected Energy-132.5348 eV
Uncorrected energy = -118.1248 eV
Composition-based energy adjustment (-0.503 eV/atom x 14.0 atoms) = -7.0420 eV
Composition-based energy adjustment (-0.614 eV/atom x 12.0 atoms) = -7.3680 eV
Corrected energy = -132.5348 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)