material

Al2Te3

ID:

mp-29502

DOI:

10.17188/1203976


Tags: Aluminium telluride - beta

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.451 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.96 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.838 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2W (mp-22693) <1 1 0> <0 1 0> 0.018 111.6
CdS (mp-672) <1 1 0> <0 1 1> 0.020 147.0
MgF2 (mp-1249) <1 1 0> <0 1 0> 0.020 223.2
Cu (mp-30) <1 1 0> <0 1 0> 0.023 111.6
Au (mp-81) <1 1 0> <0 1 1> 0.033 147.0
Te2W (mp-22693) <0 0 1> <0 0 1> 0.036 286.9
GdScO3 (mp-5690) <1 1 1> <0 0 1> 0.037 286.9
LaAlO3 (mp-2920) <1 0 0> <0 0 1> 0.040 286.9
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.051 286.9
Ag (mp-124) <1 1 0> <0 1 1> 0.053 147.0
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.055 191.3
LaF3 (mp-905) <1 0 1> <0 0 1> 0.071 286.9
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.072 286.9
AlN (mp-661) <1 1 1> <0 0 1> 0.076 286.9
TbScO3 (mp-31119) <1 1 1> <0 0 1> 0.086 286.9
DyScO3 (mp-31120) <1 1 1> <0 0 1> 0.128 286.9
CdWO4 (mp-19387) <1 0 1> <0 1 0> 0.129 223.2
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.144 286.9
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.146 286.9
SrTiO3 (mp-4651) <1 1 1> <0 0 1> 0.176 286.9
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.194 286.9
ZrO2 (mp-2858) <1 1 -1> <0 1 0> 0.206 223.2
GaN (mp-804) <0 0 1> <0 0 1> 0.224 286.9
C (mp-66) <1 1 0> <0 0 1> 0.227 286.9
Te2Mo (mp-602) <1 0 0> <0 1 0> 0.254 111.6
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.276 191.3
KP(HO2)2 (mp-23959) <0 1 1> <0 1 0> 0.278 111.6
YAlO3 (mp-3792) <1 1 0> <0 1 0> 0.294 111.6
Cu (mp-30) <1 0 0> <0 1 0> 0.307 223.2
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.343 95.6
Ga2O3 (mp-886) <1 0 1> <0 1 0> 0.421 223.2
LiNbO3 (mp-3731) <1 0 0> <0 1 0> 0.444 223.2
NdGaO3 (mp-3196) <1 1 1> <0 0 1> 0.451 286.9
MoS2 (mp-1434) <1 0 0> <0 0 1> 0.544 286.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
3 1 1 0 -0 0
1 17 7 0 0 0
1 7 45 0 0 0
0 0 0 15 0 0
-0 0 0 0 1 0
0 0 0 0 0 1
Compliance Tensor Sij (10-12Pa-1)
434.3 -38.3 -2.3 0 151.3 0
-38.3 67.5 -9.5 0 -28.6 0
-2.3 -9.5 23.9 0 -1.1 0
0 0 0 66.6 0 -7.2
151.3 -28.6 -1.1 0 1152 0
0 0 0 -7.2 0 982.6
Shear Modulus GV
7 GPa
Bulk Modulus KV
9 GPa
Shear Modulus GR
2 GPa
Bulk Modulus KR
2 GPa
Shear Modulus GVRH
4 GPa
Bulk Modulus KVRH
6 GPa
Elastic Anisotropy
18.81
Poisson's Ratio
0.20

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Rb2Hg3Te4 (mp-29107) 0.6407 0.000 3
GeAsSe (mp-29249) 0.7358 0.000 3
RbCuSe4 (mp-18365) 0.6784 0.000 3
LiGa3Te5 (mp-33338) 0.6939 0.004 3
CsCuSe4 (mp-17095) 0.6631 0.000 3
Cu2As4S3Cl2 (mp-560845) 0.5253 0.029 4
K2Li2FeO4 (mp-25751) 0.7285 0.057 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Te
Final Energy/Atom
-3.8355 eV
Corrected Energy
-153.4205 eV
-153.4205 eV = -153.4205 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 406353
Submitted by
User remarks:
  • Aluminium telluride - beta

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)