Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.015 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.415 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 313.9 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 198.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 143.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 201.4 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 237.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 251.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 143.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 201.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 237.3 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 198.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 143.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 201.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 100.7 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 118.7 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 188.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 313.9 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 133.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 313.9 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 125.5 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 313.9 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 313.9 |
C (mp-66) | <1 1 0> | <1 0 -1> | 143.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 237.3 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 313.9 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 251.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 1> | 237.3 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 188.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 188.3 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 313.9 |
Au (mp-81) | <1 0 0> | <0 1 0> | 188.3 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 313.9 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 133.8 |
C (mp-48) | <1 0 0> | <1 0 0> | 133.8 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 313.9 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 313.9 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 188.3 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 313.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 313.9 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 133.8 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 188.3 |
MgF2 (mp-1249) | <1 0 1> | <0 1 0> | 313.9 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 251.1 |
ZnO (mp-2133) | <1 0 0> | <1 1 -1> | 156.7 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 313.9 |
Ge (mp-32) | <1 0 0> | <1 1 1> | 198.6 |
Ge (mp-32) | <1 1 0> | <1 0 -1> | 143.6 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 1> | 188.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf(TlTe)4 (mp-984696) | 0.5778 | 0.000 | 3 |
Ti(CrS2)2 (mp-676144) | 0.5485 | 0.262 | 3 |
Na3(FeSe2)2 (mp-505443) | 0.5905 | 0.121 | 3 |
Rb2ZrTe3 (mp-29603) | 0.3789 | 0.000 | 3 |
Ca3(AlAs2)2 (mp-28304) | 0.5219 | 0.118 | 3 |
RbHfAgTe3 (mp-9780) | 0.7293 | 0.000 | 4 |
Li5FeNi3O8 (mp-765057) | 0.7266 | 0.269 | 4 |
Na2Zr(CuS2)2 (mp-556536) | 0.7067 | 0.000 | 4 |
ReB (mp-28893) | 0.6563 | 0.351 | 2 |
Ge3Ru2 (mp-21945) | 0.5948 | 0.000 | 2 |
Fe7S8 (mp-556435) | 0.6481 | 0.137 | 2 |
Re3P4 (mp-1474) | 0.4763 | 0.000 | 2 |
MgSi2 (mp-1073644) | 0.6453 | 0.164 | 2 |
Li10Ti2Mn3Co3O16 (mp-779764) | 0.7410 | 0.458 | 5 |
Li10Cr3Co2Ni3O16 (mp-778771) | 0.7454 | 0.263 | 5 |
Li10Ti2Fe3Co3O16 (mp-778830) | 0.7391 | 0.093 | 5 |
Li10Ti2Mn3Ni3O16 (mp-777713) | 0.7018 | 0.118 | 5 |
Li10Mn2Fe3Co3O16 (mp-777706) | 0.7480 | 0.092 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Zr_sv Te |
Final Energy/Atom-4.3818 eV |
Corrected Energy-105.1629 eV
-105.1629 eV = -105.1629 eV (uncorrected energy)
|