Final Magnetic Moment0.335 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.147 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.026 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV3Sb + Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 237.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 290.3 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 113.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 26.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 290.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 211.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 26.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 79.2 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 132.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 158.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 316.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 52.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 316.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 211.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 369.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 211.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 211.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 237.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 264.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 237.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 290.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 343.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 343.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 369.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 105.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 290.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 343.1 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 184.8 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 211.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 132.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 316.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 79.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 79.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 343.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 316.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 237.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 316.7 |
MoS2 (mp-1434) | <1 1 1> | <1 0 1> | 116.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 343.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 113.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 184.8 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 79.2 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 226.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 316.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 132.0 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 232.7 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 226.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 105.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 105.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 26.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
200 | 88 | 41 | -29 | 0 | 0 |
88 | 200 | 41 | 29 | 0 | 0 |
41 | 41 | 164 | 0 | 0 | 0 |
-29 | 29 | 0 | 14 | 0 | 0 |
0 | 0 | 0 | 0 | 14 | -29 |
0 | 0 | 0 | 0 | -29 | 56 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
-35.6 | 39.3 | -0.9 | -159.9 | 0 | 0 |
39.3 | -35.6 | -0.9 | 159.9 | 0 | 0 |
-0.9 | -0.9 | 6.6 | 0 | 0 | 0 |
-159.9 | 159.9 | 0 | -610.3 | 0 | 0 |
0 | 0 | 0 | 0 | -610.3 | -319.8 |
0 | 0 | 0 | 0 | -319.8 | -149.7 |
Shear Modulus GV43 GPa |
Bulk Modulus KV101 GPa |
Shear Modulus GR-3 GPa |
Bulk Modulus KR97 GPa |
Shear Modulus GVRH20 GPa |
Bulk Modulus KVRH99 GPa |
Elastic Anisotropy-69.86 |
Poisson's Ratio0.41 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: V_pv Sb |
Final Energy/Atom-7.2478 eV |
Corrected Energy-72.4780 eV
-72.4780 eV = -72.4780 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)