Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.320 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.011 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi15Ge4 + Li9Ge4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmmm [65] |
Hall-C 2 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 0> | 216.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 118.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 330.4 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 121.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 206.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 243.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 216.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 165.2 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 247.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 296.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 289.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 165.2 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 330.4 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 135.5 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 144.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 165.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 118.5 |
KCl (mp-23193) | <1 1 1> | <0 1 0> | 289.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 118.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 82.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 82.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 247.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 296.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 330.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 177.8 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 121.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 165.2 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 257.4 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 330.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 243.7 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 289.1 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 289.0 |
BN (mp-984) | <0 0 1> | <1 1 0> | 289.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 206.5 |
BN (mp-984) | <1 0 0> | <0 1 0> | 330.4 |
BN (mp-984) | <1 1 0> | <0 1 0> | 206.5 |
BN (mp-984) | <1 1 1> | <0 1 0> | 206.5 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 1> | 128.7 |
Al (mp-134) | <1 0 0> | <0 1 0> | 82.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 247.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 118.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 296.4 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 121.9 |
TeO2 (mp-2125) | <0 1 1> | <1 0 0> | 296.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 296.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 177.8 |
LiTaO3 (mp-3666) | <1 1 0> | <0 1 1> | 128.7 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 165.2 |
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 296.4 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 296.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2TbO3 (mp-686281) | 0.6958 | 0.279 | 3 |
RbMg6Mo (mp-1100163) | 0.7186 | 0.523 | 3 |
MnGaNi2 (mp-604537) | 0.6995 | 0.029 | 3 |
LiMg (mp-976262) | 0.6466 | 0.028 | 2 |
Li7Sn2 (mp-30767) | 0.2284 | 0.000 | 2 |
Li9Al4 (mp-568404) | 0.4671 | 0.006 | 2 |
V4Zn5 (mp-30883) | 0.6414 | 0.000 | 2 |
Li7Sn3 (mp-30768) | 0.5765 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ge_d |
Final Energy/Atom-2.8309 eV |
Corrected Energy-50.9562 eV
-50.9562 eV = -50.9562 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)