Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.588 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 296.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 111.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 185.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 185.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 262.2 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 314.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 148.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 148.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 296.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 333.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 333.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 37.1 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 64.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 296.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 209.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 259.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 64.2 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 321.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 259.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 333.7 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 52.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 148.3 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 262.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 333.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 111.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 148.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 192.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 185.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 209.8 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 256.9 |
BN (mp-984) | <1 1 1> | <1 1 0> | 262.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 185.4 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 185.4 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 185.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 296.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 185.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 148.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 1> | 128.4 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 185.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 259.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 222.5 |
BN (mp-984) | <1 1 0> | <1 1 1> | 64.2 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 259.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 296.6 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 209.8 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 185.4 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 185.4 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 157.3 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 74.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 37.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
128 | 118 | 118 | 0 | 0 | 0 |
118 | 128 | 118 | 0 | 0 | 0 |
118 | 118 | 128 | 0 | 0 | 0 |
0 | 0 | 0 | 65 | 0 | 0 |
0 | 0 | 0 | 0 | 65 | 0 |
0 | 0 | 0 | 0 | 0 | 65 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
66.3 | -31.8 | -31.8 | 0 | 0 | 0 |
-31.8 | 66.3 | -31.8 | 0 | 0 | 0 |
-31.8 | -31.8 | 66.3 | 0 | 0 | 0 |
0 | 0 | 0 | 15.4 | 0 | 0 |
0 | 0 | 0 | 0 | 15.4 | 0 |
0 | 0 | 0 | 0 | 0 | 15.4 |
Shear Modulus GV41 GPa |
Bulk Modulus KV121 GPa |
Shear Modulus GR11 GPa |
Bulk Modulus KR121 GPa |
Shear Modulus GVRH26 GPa |
Bulk Modulus KVRH121 GPa |
Elastic Anisotropy13.01 |
Poisson's Ratio0.40 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnAlCu2 (mp-3574) | 0.0000 | 0.041 | 3 |
Li2CuSn (mp-30591) | 0.0000 | 0.000 | 3 |
Mn2CoSn (mp-22465) | 0.0000 | 0.182 | 3 |
MgZnAg2 (mp-11236) | 0.0000 | 0.000 | 3 |
ErInPd2 (mp-11371) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.096 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Li3Tl (mp-7396) | 0.0000 | 0.000 | 2 |
Li3Bi (mp-23222) | 0.0000 | 0.000 | 2 |
BiF3 (mp-23301) | 0.0000 | 0.271 | 2 |
GdMg3 (mp-20534) | 0.0000 | 0.042 | 2 |
DyMg3 (mp-1546) | 0.0000 | 0.000 | 2 |
Sr (mp-95) | 0.0000 | 0.013 | 1 |
Dy (mp-10751) | 0.0000 | 0.147 | 1 |
Lu (mp-10190) | 0.0000 | 0.132 | 1 |
Na (mp-127) | 0.0000 | 0.002 | 1 |
La (mp-10023) | 0.0000 | 0.134 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ge_d Pd |
Final Energy/Atom-4.8074 eV |
Corrected Energy-19.2295 eV
Uncorrected energy = -19.2295 eV
Corrected energy = -19.2295 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)