Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.116 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.159 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density0.83 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToH4C + B4C + B10H11C2 |
Band Gap4.723 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 -1> | 229.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 276.7 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 229.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 325.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 113.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 100.5 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 325.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 256.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 325.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 325.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 276.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 325.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 221.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 252.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 260.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 260.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 227.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 256.1 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 256.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 256.1 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 325.0 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 276.7 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 252.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 65.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 325.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 332.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 195.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 221.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 332.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 332.0 |
BN (mp-984) | <1 0 0> | <0 1 0> | 332.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 227.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 221.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 113.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 276.7 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 276.7 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 130.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 -1> | 100.5 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 256.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 195.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 195.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 260.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 325.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 113.7 |
C (mp-66) | <1 0 0> | <0 1 1> | 256.1 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 221.3 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 113.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 1> | 155.6 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 113.7 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 325.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsB9H14 (mp-27590) | 0.5242 | 0.064 | 3 |
Cr(B3H8)2 (mp-567148) | 0.6438 | 0.051 | 3 |
B5H6Br (mp-30977) | 0.5099 | 0.000 | 3 |
CsB3H8 (mp-28582) | 0.6018 | 0.008 | 3 |
B9H11C2 (mp-28052) | 0.5107 | 0.050 | 3 |
FeH2Cl5O3 (mp-735518) | 0.5524 | 0.530 | 4 |
KNa2AlH6 (mp-600151) | 0.7117 | 0.154 | 4 |
MoSe2Cl4O (mp-671913) | 0.7326 | 0.121 | 4 |
B2H3 (mp-27876) | 0.5430 | 0.035 | 2 |
B3H5 (mp-29721) | 0.3923 | 0.038 | 2 |
B7H10 (mp-27820) | 0.4561 | 0.032 | 2 |
B9H11 (mp-29654) | 0.5219 | 0.000 | 2 |
B5H7 (mp-706630) | 0.4863 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: B H C |
Final Energy/Atom-5.1940 eV |
Corrected Energy-290.8664 eV
-290.8664 eV = -290.8664 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)