material

Si5Pt6

ID:

mp-29661

DOI:

10.17188/1204145


Tags: Platinum silicide (6/5) Platinum silicon (6/5)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.680 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
12.65 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/m [11]
Hall
-P 2yb
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 43283 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <1 0 0> <1 0 -1> 0.007 174.8
GaSb (mp-1156) <1 0 0> <0 0 1> 0.012 154.9
PbSe (mp-2201) <1 0 0> <0 0 1> 0.015 154.9
CdSe (mp-2691) <1 0 0> <0 0 1> 0.019 154.9
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.028 199.2
CdWO4 (mp-19387) <0 1 0> <0 0 1> 0.034 132.8
LiNbO3 (mp-3731) <1 0 0> <1 0 0> 0.035 221.1
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.046 110.7
ZnO (mp-2133) <1 1 1> <0 0 1> 0.078 221.3
BaF2 (mp-1029) <1 1 0> <0 0 1> 0.079 110.7
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.082 304.0
SiC (mp-8062) <1 0 0> <0 0 1> 0.089 154.9
SiC (mp-11714) <0 0 1> <0 0 1> 0.095 66.4
GaN (mp-804) <0 0 1> <0 0 1> 0.096 287.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.097 66.4
PbSe (mp-2201) <1 1 0> <0 0 1> 0.098 110.7
Au (mp-81) <1 0 0> <1 0 0> 0.103 331.7
SiC (mp-8062) <1 1 1> <0 0 1> 0.103 66.4
SrTiO3 (mp-4651) <1 1 1> <1 0 0> 0.114 276.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.118 177.1
C (mp-48) <1 0 1> <1 0 0> 0.127 276.4
WS2 (mp-224) <1 1 0> <1 0 -1> 0.131 233.0
C (mp-66) <1 0 0> <0 0 1> 0.136 88.5
Bi2Te3 (mp-34202) <0 0 1> <1 0 0> 0.138 276.4
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.138 22.1
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.139 276.4
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.144 177.1
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.145 154.9
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.147 154.9
BaTiO3 (mp-5986) <1 0 1> <1 0 0> 0.147 276.4
GaSb (mp-1156) <1 1 0> <0 0 1> 0.151 110.7
ZnO (mp-2133) <0 0 1> <0 0 1> 0.153 177.1
AlN (mp-661) <1 0 1> <0 0 1> 0.155 287.7
AlN (mp-661) <1 1 0> <0 1 1> 0.156 298.8
C (mp-48) <0 0 1> <0 0 1> 0.159 199.2
InAs (mp-20305) <1 0 0> <0 0 1> 0.173 154.9
BaF2 (mp-1029) <1 1 1> <1 0 0> 0.186 276.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.192 354.1
LaF3 (mp-905) <1 0 0> <0 0 1> 0.193 265.6
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.193 287.7
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.194 287.7
CdSe (mp-2691) <1 1 0> <0 0 1> 0.202 110.7
TiO2 (mp-2657) <1 0 0> <1 0 -1> 0.207 291.3
GaN (mp-804) <1 0 0> <1 0 0> 0.212 221.1
AlN (mp-661) <1 0 0> <0 0 1> 0.226 154.9
Te2W (mp-22693) <1 0 1> <0 0 1> 0.230 199.2
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.244 199.2
CdS (mp-672) <1 0 1> <1 0 -1> 0.245 291.3
ZrO2 (mp-2858) <0 1 0> <1 0 1> 0.253 304.0
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.259 177.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
337 126 127 0 18 0
126 230 150 0 -2 0
127 150 271 0 16 0
0 0 0 80 0 -8
18 -2 16 0 67 0
0 0 0 -8 0 68
Compliance Tensor Sij (10-12Pa-1)
4 -1.6 -0.9 0 -0.9 0
-1.6 7.5 -3.5 0 1.5 0
-0.9 -3.5 6.2 0 -1.4 0
0 0 0 12.7 0 1.5
-0.9 1.5 -1.4 0 15.6 0
0 0 0 1.5 0 14.9
Shear Modulus GV
72 GPa
Bulk Modulus KV
183 GPa
Shear Modulus GR
67 GPa
Bulk Modulus KR
179 GPa
Shear Modulus GVRH
69 GPa
Bulk Modulus KVRH
181 GPa
Elastic Anisotropy
0.39
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ag5Te2Cl (mp-569467) 0.7298 0.000 3
LiYb8Ge13 (mp-680614) 0.7397 0.325 3
Hf5CoAs3 (mp-505333) 0.7081 0.000 3
Sc5(NiTe)2 (mp-29769) 0.6791 0.000 3
Mg2Si3 (mp-1073021) 0.7009 0.194 2
Mg2Si3 (mp-1073166) 0.7078 0.209 2
Mg2Si3 (mp-1073176) 0.6929 0.165 2
Mg2Si3 (mp-1073232) 0.6088 0.184 2
Mg3Si4 (mp-1075263) 0.7194 0.198 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Si Pt
Final Energy/Atom
-6.4565 eV
Corrected Energy
-142.0424 eV
Uncorrected energy = -142.0424 eV Corrected energy = -142.0424 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43283
  • 649605
Submitted by
User remarks:
  • Platinum silicon (6/5)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)