material

Al2B2Ru3

ID:

mp-29674

DOI:

10.17188/1204154


Tags: Aluminum ruthenium boride (2/3/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.471 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.079 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Al3(BRu2)2 + B2Ru
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmmm [65]
Hall
-C 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 43843 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LiGaO2 (mp-5854) <0 1 1> <1 0 1> 0.000 301.6
PbSe (mp-2201) <1 1 1> <0 1 0> 0.018 134.1
InP (mp-20351) <1 1 0> <1 0 1> 0.020 150.8
GaSb (mp-1156) <1 1 1> <0 1 0> 0.020 134.1
CdSe (mp-2691) <1 1 1> <0 1 0> 0.030 134.1
Ga2O3 (mp-886) <0 1 0> <0 1 0> 0.038 71.5
LiGaO2 (mp-5854) <1 1 1> <0 1 0> 0.045 223.6
Ag (mp-124) <1 1 1> <0 1 0> 0.046 89.4
GaP (mp-2490) <1 1 1> <0 1 0> 0.055 313.0
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.058 314.7
Si (mp-149) <1 1 1> <0 1 0> 0.069 313.0
CdTe (mp-406) <1 0 0> <1 0 0> 0.074 262.3
CeO2 (mp-20194) <1 1 1> <0 1 0> 0.076 313.0
InSb (mp-20012) <1 0 0> <1 0 0> 0.090 262.3
BN (mp-984) <1 0 0> <0 1 0> 0.095 116.3
AlN (mp-661) <1 1 1> <0 1 0> 0.107 169.9
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.109 262.3
CaF2 (mp-2741) <1 1 1> <0 1 0> 0.110 313.0
Te2Mo (mp-602) <1 0 0> <0 1 0> 0.110 330.9
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.115 262.3
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.118 314.7
Ni (mp-23) <1 1 0> <0 1 0> 0.121 241.4
YVO4 (mp-19133) <1 1 0> <0 1 0> 0.123 196.7
Au (mp-81) <1 1 1> <0 1 0> 0.125 89.4
TbScO3 (mp-31119) <1 1 0> <1 0 0> 0.130 314.7
NdGaO3 (mp-3196) <1 1 1> <0 1 0> 0.134 205.7
GaN (mp-804) <1 1 1> <0 1 0> 0.136 152.0
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.136 75.9
LaF3 (mp-905) <0 0 1> <1 1 1> 0.145 227.8
ZnTe (mp-2176) <1 1 1> <0 1 0> 0.166 134.1
SrTiO3 (mp-4651) <1 1 1> <0 1 0> 0.176 277.2
PbS (mp-21276) <1 1 0> <1 0 1> 0.182 150.8
InAs (mp-20305) <1 1 1> <0 1 0> 0.192 134.1
ZrO2 (mp-2858) <1 1 1> <0 1 0> 0.194 205.7
CdS (mp-672) <0 0 1> <1 1 1> 0.195 75.9
NdGaO3 (mp-3196) <0 0 1> <0 1 0> 0.212 152.0
TiO2 (mp-390) <1 0 0> <0 1 0> 0.251 187.8
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.251 17.9
Te2Mo (mp-602) <1 0 1> <0 1 0> 0.252 330.9
GdScO3 (mp-5690) <0 1 1> <0 1 0> 0.290 330.9
ZrO2 (mp-2858) <0 1 0> <0 1 0> 0.291 169.9
YAlO3 (mp-3792) <1 1 0> <0 1 0> 0.293 223.6
LiGaO2 (mp-5854) <0 0 1> <0 1 0> 0.295 169.9
SiO2 (mp-6930) <1 1 0> <0 1 0> 0.302 241.4
CsI (mp-614603) <1 0 0> <1 0 0> 0.326 314.7
MgO (mp-1265) <1 1 0> <1 0 1> 0.350 75.4
InAs (mp-20305) <1 1 0> <0 1 0> 0.353 53.7
BaF2 (mp-1029) <1 1 1> <0 1 0> 0.363 134.1
Mg (mp-153) <1 1 1> <0 1 0> 0.365 152.0
TiO2 (mp-2657) <1 0 1> <0 1 0> 0.366 152.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
357 195 139 0 0 0
195 318 149 0 0 0
139 149 430 0 0 0
0 0 0 100 0 0
0 0 0 0 132 0
0 0 0 0 0 92
Compliance Tensor Sij (10-12Pa-1)
4.3 -2.4 -0.6 0 0 0
-2.4 5.1 -1 0 0 0
-0.6 -1 2.9 0 0 0
0 0 0 10 0 0
0 0 0 0 7.6 0
0 0 0 0 0 10.9
Shear Modulus GV
106 GPa
Bulk Modulus KV
230 GPa
Shear Modulus GR
100 GPa
Bulk Modulus KR
229 GPa
Shear Modulus GVRH
103 GPa
Bulk Modulus KVRH
230 GPa
Elastic Anisotropy
0.32
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al B Ru_pv
Final Energy/Atom
-7.4245 eV
Corrected Energy
-51.9716 eV
-51.9716 eV = -51.9716 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43843
Submitted by
User remarks:
  • Aluminum ruthenium boride (2/3/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)