Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.585 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.457 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 204.0 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 272.0 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 272.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 136.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 272.0 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 272.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 -1> | 177.0 |
BN (mp-984) | <1 0 1> | <0 1 0> | 204.0 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 272.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 161.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 272.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 161.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 155.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.5 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 272.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 272.0 |
C (mp-66) | <1 0 0> | <0 1 0> | 272.0 |
C (mp-66) | <1 1 0> | <0 1 0> | 272.0 |
C (mp-66) | <1 1 1> | <1 0 -1> | 177.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 139.5 |
Mg (mp-153) | <1 0 1> | <1 1 -1> | 189.6 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 272.0 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 272.0 |
GaP (mp-2490) | <1 1 1> | <0 1 0> | 272.0 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 1> | 155.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 139.5 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 272.0 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 161.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 139.5 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 272.0 |
NdGaO3 (mp-3196) | <1 1 1> | <0 0 1> | 139.5 |
Si (mp-149) | <1 0 0> | <0 1 0> | 272.0 |
Si (mp-149) | <1 1 1> | <0 1 0> | 272.0 |
CdSe (mp-2691) | <1 1 0> | <0 1 0> | 272.0 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 272.0 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 0> | 272.0 |
C (mp-48) | <1 0 0> | <1 1 0> | 174.8 |
C (mp-48) | <1 0 1> | <0 1 0> | 204.0 |
NaCl (mp-22862) | <1 1 1> | <0 1 0> | 272.0 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 204.0 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 -1> | 177.0 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 -1> | 177.0 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 136.0 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 204.0 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 0> | 204.0 |
CdWO4 (mp-19387) | <1 1 1> | <0 1 1> | 155.2 |
GaSb (mp-1156) | <1 1 0> | <0 1 0> | 272.0 |
SrTiO3 (mp-4651) | <0 0 1> | <0 1 0> | 272.0 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 272.0 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 272.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Rb3Ti3Te11 (mp-505639) | 0.7466 | 0.000 | 3 |
Rb3Ti3Te11 (mp-580680) | 0.7487 | 0.000 | 3 |
Mg2Si3 (mp-1073122) | 0.7100 | 0.239 | 2 |
MgSi2 (mp-1073590) | 0.7447 | 0.194 | 2 |
Ag2S (mp-32868) | 0.6383 | 0.052 | 2 |
CeSe2 (mp-1080353) | 0.7146 | 0.091 | 2 |
Mg5Si6 (mp-1075569) | 0.6742 | 0.204 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ag S |
Final Energy/Atom-3.5808 eV |
Corrected Energy-213.7945 eV
-213.7945 eV = -200.5253 eV (uncorrected energy) - 13.2692 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)