Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.694 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.230 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 297.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 91.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 223.4 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 141.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 131.1 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 223.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 91.5 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 274.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 131.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 131.1 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 223.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 223.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 262.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 274.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 262.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 91.5 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 141.0 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 274.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 223.4 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 141.0 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 141.0 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 223.4 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 223.4 |
C (mp-66) | <1 0 0> | <0 1 0> | 297.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 -1> | 159.4 |
Mg (mp-153) | <0 0 1> | <1 0 -1> | 141.0 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 1 0> | 223.4 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 0> | 131.1 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 0> | 131.1 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 91.5 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 274.6 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 91.5 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 -1> | 159.4 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 262.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 223.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 -1> | 159.4 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 223.4 |
SiC (mp-11714) | <1 1 1> | <0 1 0> | 223.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 262.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 1> | 236.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 262.1 |
WS2 (mp-224) | <0 0 1> | <1 0 -1> | 141.0 |
C (mp-48) | <1 0 1> | <0 1 1> | 118.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 223.4 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 223.4 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 223.4 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 223.4 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 274.6 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 274.6 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 0> | 223.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbSeCl9 (mp-28985) | 0.2431 | 0.000 | 3 |
Mo(SeCl6)2 (mp-568726) | 0.4917 | 0.014 | 3 |
Os(SeCl6)2 (mp-582444) | 0.4890 | 0.002 | 3 |
Te2WCl6 (mp-662513) | 0.4040 | 0.022 | 3 |
TeWBr9 (mp-29715) | 0.1189 | 0.008 | 3 |
RbAsOF4 (mp-17337) | 0.7114 | 0.000 | 4 |
KAsOF4 (mp-17539) | 0.6253 | 0.000 | 4 |
TeAs(SeF3)2 (mp-651161) | 0.6947 | 0.109 | 4 |
AsS(IF3)2 (mp-557628) | 0.7082 | 0.000 | 4 |
SbSNCl5 (mp-559738) | 0.7012 | 0.095 | 4 |
ReCl5 (mp-27645) | 0.5659 | 0.054 | 2 |
TcCl4 (mp-27780) | 0.5672 | 0.000 | 2 |
TeI4 (mp-651155) | 0.5682 | 0.002 | 2 |
TcBr4 (mp-570480) | 0.5418 | 0.024 | 2 |
Rb9O2 (mp-27561) | 0.4259 | 0.000 | 2 |
HfMo2Se8(Cl7O)2 (mp-629742) | 0.7499 | 0.026 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv Te Br |
Final Energy/Atom-3.3967 eV |
Corrected Energy-74.7276 eV
-74.7276 eV = -74.7276 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)