Final Magnetic Moment3.027 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.257 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.036 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoCl2 + BaCl2 |
Band Gap0.264 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 211.6 |
LaAlO3 (mp-2920) | <1 1 0> | <0 1 0> | 119.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 176.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 119.3 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 141.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 259.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 129.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 184.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 226.9 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 159.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 184.4 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 184.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 226.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 226.9 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 141.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 129.9 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 184.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 226.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 129.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 259.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 226.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 129.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 129.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 184.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 259.8 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 119.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 259.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 1> | 141.2 |
Al (mp-134) | <1 1 0> | <1 0 1> | 184.4 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 119.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 302.5 |
Al (mp-134) | <1 0 0> | <1 0 0> | 129.9 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 141.2 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 238.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 1> | 141.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 226.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 226.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 184.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 129.9 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 259.8 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 226.9 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 1> | 184.4 |
Ni (mp-23) | <1 0 0> | <1 1 -1> | 159.5 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 259.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 129.9 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 119.3 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 -1> | 159.5 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 141.2 |
C (mp-48) | <1 0 0> | <1 0 -1> | 211.6 |
MoSe2 (mp-1634) | <1 0 1> | <1 0 0> | 259.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ScCl7 (mp-573888) | 0.5921 | 0.026 | 3 |
Ba2CaI6 (mp-766288) | 0.5415 | 0.035 | 3 |
Ba2LaCl7 (mp-773111) | 0.5476 | 0.076 | 3 |
Ba2YCl7 (mp-768983) | 0.5704 | 0.039 | 3 |
Ba2YBr7 (mp-768373) | 0.5496 | 0.035 | 3 |
Pr2SbO5F (mp-554138) | 0.5493 | 0.000 | 4 |
Te2Mo3Se7Br10 (mp-645663) | 0.7158 | 0.000 | 4 |
NaSr2CrF8 (mp-653560) | 0.6898 | 0.085 | 4 |
BaMgBiF7 (mvc-10353) | 0.7414 | 0.052 | 4 |
NaSrAlF6 (mp-14722) | 0.7355 | 0.000 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Co Cl |
Final Energy/Atom-4.3090 eV |
Corrected Energy-169.8583 eV
Uncorrected energy = -155.1223 eV
Composition-based energy adjustment (-0.614 eV/atom x 24.0 atoms) = -14.7360 eV
Corrected energy = -169.8583 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)