Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.439 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.87 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPbBrF + PbF2 |
Band Gap4.063 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6 [174] |
HallP 6 |
Point Group6 |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 286.8 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 298.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 286.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 295.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 127.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 298.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 213.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 213.0 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 221.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 85.2 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 73.8 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 298.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 286.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 295.2 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 298.2 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 286.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 95.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 286.8 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 255.6 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 298.2 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 213.0 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 85.2 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 213.0 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 298.2 |
SiC (mp-11714) | <1 1 0> | <1 0 1> | 104.7 |
SiC (mp-11714) | <1 1 1> | <1 0 0> | 213.0 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 255.6 |
Au (mp-81) | <1 0 0> | <1 0 0> | 85.2 |
Au (mp-81) | <1 1 0> | <1 1 0> | 73.8 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 255.6 |
WS2 (mp-224) | <1 1 1> | <1 0 0> | 298.2 |
C (mp-48) | <0 0 1> | <1 0 0> | 340.9 |
C (mp-48) | <1 0 1> | <1 1 0> | 295.2 |
C (mp-48) | <1 1 1> | <1 0 0> | 298.2 |
NaCl (mp-22862) | <1 0 0> | <1 1 0> | 295.2 |
NaCl (mp-22862) | <1 1 1> | <1 0 0> | 170.4 |
ZrO2 (mp-2858) | <0 1 1> | <1 0 0> | 340.9 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 213.0 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 286.8 |
ZrO2 (mp-2858) | <1 0 1> | <1 1 0> | 295.2 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 221.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 298.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 298.2 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 295.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 170.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 295.2 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 213.0 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 286.8 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 295.2 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 170.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
9.95244 | -9.95244 | 0.00000 | 0.00000 | 0.00000 | 2.28756 |
2.28756 | -2.28756 | 0.00000 | 0.00000 | 0.00000 | -9.95244 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max14.44189 C/m2 |
Crystallographic Direction vmax |
---|
-4.00000 |
-1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.95 | -0.00 | 0.00 |
0.00 | 3.95 | 0.00 |
0.00 | 0.00 | 4.20 |
Dielectric Tensor εij (total) |
||
---|---|---|
226.16 | -0.00 | 0.00 |
0.00 | 226.16 | 0.00 |
0.00 | 0.00 | 33.67 |
Polycrystalline dielectric constant
εpoly∞
4.03
|
Polycrystalline dielectric constant
εpoly
162.00
|
Refractive Index n2.01 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb2Co12P7 (mp-15842) | 0.4086 | 0.000 | 3 |
Ca7(H6Cl)2 (mp-984055) | 0.4279 | 0.000 | 3 |
Sr7(H6Cl)2 (mp-23827) | 0.4307 | 0.000 | 3 |
Pb7(ClF6)2 (mp-27581) | 0.3322 | 0.011 | 3 |
Zr2Fe12P7 (mp-540809) | 0.4179 | 0.000 | 3 |
Ba6Eu(ClF6)2 (mp-556702) | 0.5513 | 0.024 | 4 |
Mg6Si5 (mp-1073921) | 0.7462 | 0.131 | 2 |
Mg3Si4 (mp-1075277) | 0.7377 | 0.188 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pb_d Br F |
Final Energy/Atom-4.6441 eV |
Corrected Energy-103.0697 eV
Uncorrected energy = -97.5257 eV
Composition-based energy adjustment (-0.462 eV/atom x 12.0 atoms) = -5.5440 eV
Corrected energy = -103.0697 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)