Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.524 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 266.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 133.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 349.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 153.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 271.8 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 133.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 116.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 230.5 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 133.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 194.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 116.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 307.3 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 307.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 271.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 271.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 194.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 116.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 116.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 38.8 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 116.5 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 349.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 230.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 153.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 194.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 271.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 76.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 271.8 |
BN (mp-984) | <1 1 1> | <1 0 0> | 307.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 116.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 271.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 194.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 271.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 271.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 194.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 194.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 138.6 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 266.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 194.1 |
Al (mp-134) | <1 1 0> | <1 1 1> | 138.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 116.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 307.3 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 307.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 194.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 155.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 271.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 116.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 1> | 258.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 271.8 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 194.1 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
402 | 62 | 95 | -0 | 0 | 0 |
62 | 402 | 95 | 0 | 0 | 0 |
95 | 95 | 329 | 0 | 0 | 0 |
-0 | 0 | 0 | 93 | 0 | 0 |
0 | 0 | 0 | 0 | 93 | -0 |
0 | 0 | 0 | 0 | -0 | 170 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
2.7 | -0.2 | -0.7 | 0 | 0 | 0 |
-0.2 | 2.7 | -0.7 | 0 | 0 | 0 |
-0.7 | -0.7 | 3.4 | 0 | 0 | 0 |
0 | 0 | 0 | 10.8 | 0 | 0 |
0 | 0 | 0 | 0 | 10.8 | 0 |
0 | 0 | 0 | 0 | 0 | 5.9 |
Shear Modulus GV130 GPa |
Bulk Modulus KV182 GPa |
Shear Modulus GR121 GPa |
Bulk Modulus KR181 GPa |
Shear Modulus GVRH125 GPa |
Bulk Modulus KVRH181 GPa |
Elastic Anisotropy0.39 |
Poisson's Ratio0.22 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeB2C (mp-8667) | 0.0486 | 0.000 | 3 |
UB2C (mp-11332) | 0.2146 | 0.079 | 3 |
PuB2C (mp-1095228) | 0.3664 | 0.259 | 3 |
NpB2C (mp-1095351) | 0.2049 | 0.070 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Th B C |
Final Energy/Atom-8.0238 eV |
Corrected Energy-96.2856 eV
Uncorrected energy = -96.2856 eV
Corrected energy = -96.2856 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)