Final Magnetic Moment0.125 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.716 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
SiC (mp-7631) | <0 0 1> | <1 1 0> | 0.008 | 191.5 |
SiC (mp-11714) | <0 0 1> | <1 1 0> | 0.009 | 191.5 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 1> | 0.011 | 299.5 |
BN (mp-984) | <1 1 0> | <1 0 0> | 0.014 | 333.7 |
ZnO (mp-2133) | <1 1 0> | <0 1 1> | 0.015 | 211.8 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 0.021 | 299.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 0.023 | 179.7 |
C (mp-48) | <1 0 1> | <1 0 0> | 0.068 | 282.4 |
TiO2 (mp-390) | <1 0 0> | <1 0 -1> | 0.071 | 112.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 0.073 | 256.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 0.079 | 179.7 |
C (mp-48) | <1 1 1> | <1 0 0> | 0.081 | 333.7 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 0.108 | 179.7 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 0.110 | 156.0 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 0.124 | 154.0 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 0.126 | 102.7 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 0.135 | 205.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 0.138 | 179.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 0.138 | 333.7 |
SiC (mp-7631) | <1 1 0> | <1 0 1> | 0.142 | 239.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 0.145 | 119.8 |
SiC (mp-8062) | <1 1 0> | <1 0 1> | 0.148 | 239.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 0.151 | 299.5 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 0.153 | 191.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 0.153 | 154.0 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 0.156 | 359.4 |
NaCl (mp-22862) | <1 1 0> | <1 0 1> | 0.156 | 179.7 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 0.162 | 299.5 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 0> | 0.163 | 333.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 0.167 | 231.1 |
MgAl2O4 (mp-3536) | <1 1 1> | <1 0 0> | 0.167 | 231.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 0.169 | 231.1 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 0.172 | 231.1 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 0.173 | 77.0 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 0.173 | 77.0 |
MoSe2 (mp-1634) | <1 1 0> | <1 0 1> | 0.176 | 179.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 0.181 | 77.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 0.186 | 280.1 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 0.189 | 231.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 0.190 | 231.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 0.190 | 179.7 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 1> | 0.191 | 179.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 0.191 | 276.7 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 0.192 | 260.0 |
NaCl (mp-22862) | <1 1 1> | <1 0 0> | 0.197 | 333.7 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 1> | 0.198 | 179.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 0.200 | 205.4 |
Ge (mp-32) | <1 1 0> | <1 0 -1> | 0.203 | 280.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 0.206 | 333.7 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 0.207 | 179.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
68 | 14 | 25 | 0 | 10 | 0 |
14 | 86 | 24 | 0 | 0 | 0 |
25 | 24 | 91 | 0 | 19 | 0 |
0 | 0 | 0 | 28 | 0 | -2 |
10 | 0 | 19 | 0 | 29 | 0 |
0 | 0 | 0 | -2 | 0 | 18 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
16.8 | -1.9 | -3.4 | 0 | -3.7 | 0 |
-1.9 | 12.9 | -3.5 | 0 | 2.9 | 0 |
-3.4 | -3.5 | 14.5 | 0 | -8.3 | 0 |
0 | 0 | 0 | 36 | 0 | 3.2 |
-3.7 | 2.9 | -8.3 | 0 | 41.6 | 0 |
0 | 0 | 0 | 3.2 | 0 | 57.3 |
Shear Modulus GV27 GPa |
Bulk Modulus KV41 GPa |
Shear Modulus GR24 GPa |
Bulk Modulus KR37 GPa |
Shear Modulus GVRH26 GPa |
Bulk Modulus KVRH39 GPa |
Elastic Anisotropy0.65 |
Poisson's Ratio0.23 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlHO2 (mp-625420) | 0.7291 | 0.027 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv N |
Final Energy/Atom-5.5366 eV |
Corrected Energy-44.2930 eV
-44.2930 eV = -44.2930 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)