material

BaTiO3

ID:

mp-2998

DOI:

10.17188/1204413


Tags: Barium titanate High pressure experimental phase Barium titanium oxide (1/1/3) Perovskite-(Ba) Barium titanate(IV) Barium Titanate

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-3.487 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.015 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.89 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
BaTiO3
Band Gap
1.725 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 27965 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <1 0 0> 0.000 130.3
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.001 253.3
Al (mp-134) <1 0 0> <1 0 0> 0.002 16.3
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.002 197.5
Si (mp-149) <1 1 0> <1 1 0> 0.002 253.3
Al (mp-134) <1 1 0> <1 1 0> 0.002 23.0
Al (mp-134) <1 1 1> <1 1 1> 0.002 28.2
Ge(Bi3O5)4 (mp-23352) <1 0 0> <1 0 0> 0.003 211.7
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.004 16.3
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.005 23.0
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.005 28.2
Ge3(BiO3)4 (mp-23560) <1 1 1> <1 1 1> 0.006 197.5
C (mp-48) <0 0 1> <1 1 1> 0.009 84.6
ZnO (mp-2133) <0 0 1> <1 1 1> 0.011 28.2
Cu (mp-30) <1 0 0> <1 0 0> 0.011 65.1
KCl (mp-23193) <1 0 0> <1 0 0> 0.016 81.4
NaCl (mp-22862) <1 0 0> <1 0 0> 0.023 32.6
NaCl (mp-22862) <1 1 0> <1 1 0> 0.024 46.1
InAs (mp-20305) <1 1 1> <1 1 1> 0.026 197.5
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.030 230.3
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.032 146.6
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.034 207.3
ZnTe (mp-2176) <1 1 1> <1 1 1> 0.037 197.5
GaSe (mp-1943) <0 0 1> <1 1 1> 0.038 112.8
TePb (mp-19717) <1 1 0> <1 1 0> 0.043 184.3
Ni (mp-23) <1 1 0> <1 1 0> 0.047 69.1
Ni (mp-23) <1 1 1> <1 1 1> 0.047 84.6
CdS (mp-672) <0 0 1> <1 1 1> 0.066 197.5
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.091 115.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.098 146.6
MgO (mp-1265) <1 1 0> <1 1 0> 0.102 207.3
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.107 244.3
Mg (mp-153) <0 0 1> <1 1 1> 0.108 112.8
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.109 276.9
CdTe (mp-406) <1 1 0> <1 1 0> 0.116 184.3
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.118 309.4
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.119 299.4
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.121 32.6
WSe2 (mp-1821) <1 0 0> <1 1 0> 0.122 299.4
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.124 46.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.126 46.1
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.128 253.3
LiAlO2 (mp-3427) <1 0 0> <1 1 0> 0.129 230.3
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.131 211.7
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.139 325.7
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.142 46.1
InSb (mp-20012) <1 1 0> <1 1 0> 0.142 184.3
C (mp-48) <1 0 0> <1 0 0> 0.144 309.4
BaTiO3 (mp-5986) <1 1 0> <1 1 1> 0.151 169.2
Mg (mp-153) <1 0 1> <1 1 0> 0.162 322.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
282 104 104 0 0 0
104 282 104 0 0 0
104 104 282 0 0 0
0 0 0 120 0 0
0 0 0 0 120 0
0 0 0 0 0 120
Compliance Tensor Sij (10-12Pa-1)
4.4 -1.2 -1.2 0 0 0
-1.2 4.4 -1.2 0 0 0
-1.2 -1.2 4.4 0 0 0
0 0 0 8.3 0 0
0 0 0 0 8.3 0
0 0 0 0 0 8.3
Shear Modulus GV
108 GPa
Bulk Modulus KV
163 GPa
Shear Modulus GR
106 GPa
Bulk Modulus KR
163 GPa
Shear Modulus GVRH
107 GPa
Bulk Modulus KVRH
163 GPa
Elastic Anisotropy
0.11
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiAlO3 (mvc-11693) 0.0077 0.996 3
AlSnO3 (mvc-11052) 0.0049 1.319 3
MnAlO3 (mvc-15603) 0.0077 1.290 3
AlBiO3 (mvc-15476) 0.0075 1.666 3
YWO3 (mvc-14645) 0.0058 0.812 3
La2ReNiO6 (mp-1078601) 0.0155 0.288 4
Ba2ScSbO6 (mp-20709) 0.0155 2.196 4
Cs2LiYCl6 (mp-567652) 0.0154 0.000 4
Sr2GaSbO6 (mp-6065) 0.0153 0.039 4
Ba2NbFeO6 (mp-1096853) 0.0155 2.749 4
Ba3Sb2 (mp-1013582) 0.0155 0.409 2
Ca3Bi2 (mp-1013735) 0.0155 0.366 2
Ba3N2 (mp-1013528) 0.0155 0.683 2
Ca3N2 (mp-1013524) 0.0155 0.512 2
Ba3P2 (mp-1013551) 0.0155 0.446 2
BaLaMgBiO6 (mp-41414) 0.0480 0.096 5
BaLaMgNbO6 (mp-39288) 0.0625 0.090 5
SrLaNbZnO6 (mp-41918) 0.0648 0.126 5
SrLaMnCoO6 (mp-40761) 0.0402 0.247 5
Sr6Ca2MnFe7O24 (mp-1075969) 0.0408 0.021 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7271 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

Compositionally graded (Ba1-xSrx)TiO3 (BST) (x:0.00.25) thin films were grown on Pt(111)/TiO2/SiO2/Si(100) substrates using layer-by-layer pulsed laser deposition in the temperature range 550650 [...]
Lead-free positive temperature coefficient of resistivity (PTCR) ceramics of 99mol%BaTiO31mol%(Bi1/2Na1/2)TiO3 (BBNT1) and 90mol%BaTiO310mol%(Bi1/2Na1/2)TiO3 (BBNT10) were prepared by the conven [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition BaTiO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Ti_pv O
Final Energy/Atom
-7.9970 eV
Corrected Energy
-42.0917 eV
-42.0917 eV = -39.9848 eV (uncorrected energy) - 2.1069 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 252562
  • 67519
  • 56093
  • 166225
  • 186437
  • 27968
  • 27971
  • 27975
  • 29147
  • 27967
  • 28854
  • 27973
  • 154344
  • 28851
  • 27972
  • 31889
  • 28620
  • 43125
  • 29146
  • 27977
  • 31887
  • 99736
  • 31884
  • 28852
  • 100804
  • 190924
  • 290019
  • 27969
  • 29280
  • 27974
  • 28853
  • 31886
  • 95437
  • 28849
  • 28848
  • 31890
  • 29148
  • 31888
  • 31885
  • 185374
  • 27976
  • 27965
  • 27970
  • 28850
  • 187292
  • 27966
  • 67518
  • 187291

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)