Final Magnetic Moment0.043 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.499 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4132 [214] |
HallI 4bd 2c 3 |
Point Group432 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 157.8 |
Au (mp-81) | <1 0 0> | <1 0 0> | 157.8 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 157.8 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 157.8 |
C (mp-48) | <0 0 1> | <1 0 0> | 157.8 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 157.8 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 157.8 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 157.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La12Au3I13 (mp-674940) | 0.2337 | 0.001 | 3 |
La3AsI3 (mp-29997) | 0.1255 | 0.000 | 3 |
Ca3PI3 (mp-27272) | 0.2788 | 0.000 | 3 |
Gd3CCl3 (mp-28133) | 0.1080 | 0.000 | 3 |
Pr3PtI3 (mp-653855) | 0.0817 | 0.000 | 3 |
Li6AlFeO6 (mp-779415) | 0.7305 | 0.110 | 4 |
Li6AlCrO6 (mp-770562) | 0.7381 | 0.122 | 4 |
Na2GeTeO6 (mp-10340) | 0.7431 | 0.000 | 4 |
Yb2S3 (mp-619061) | 0.7025 | 0.503 | 2 |
Cd3N2 (mp-569957) | 0.7470 | 0.397 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La P I |
Final Energy/Atom-5.0405 eV |
Corrected Energy-141.1340 eV
-141.1340 eV = -141.1340 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)